SA 2.5 is, by definition a grit blast finish – so the answer is no.
Alan Denney
AKD Materials Consulting Ltd
From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Jasim Ahmed
Sent: 18 August 2015 08:00
To: Materials & Welding <material...@googlegroups.com>
Subject: [MW:23305] S.A. 2.5 surface profile
Dear experts,
I badly need to know - is it possible to create S.A. 2.5 surface profile for joint wrapping without sand blasting?
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5e6cfb73-db6b-48b1-8dbe-a7bb3f93f062%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
| Do you want only without sand blasting or without any type of blasting. Now a days sand blasting is rarely used bcoz of its environmental issues. If you want you can blast with copper slag or iron grit. But it is not possible without blasting. Sent from Yahoo Mail on Android
|
|
|
|
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1439954087.46828.YahooMailAndroidMobile%40web181306.mail.ne1.yahoo.com.
Dear experts,I badly need to know - is it possible to create S.A. 2.5 surface profile for joint wrapping without sand blasting?
--
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA%2BqLVs6Y8RETYQvfBtLTQcSqmh0v_akgchrKeG4S565iEPMQA%40mail.gmail.com.
Alan Denney
AKD Materials Consulting Ltd
From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Madhan S
Sent: 22 November 2015 04:51
To: Materials & Welding <material...@googlegroups.com>
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/38a30053-9679-4b69-baa4-448d31c24b0d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.