Dear Experts ,

Greetings,
in PQR preheat temp is 30 degree centigrade and interpass temp is 100 degreecentigrade .

what temp minimum and maximum we can mentioned in WPS .

as per sec IX decrease  greater than 55  Degree centigrade is an essential variable what does it mean ?
increase Greater than 55 is an supplementary essential variable .what temp could be in wps ?

thanks in advance .



image.png

image.png

image.png


Best Regards,
Zafar Iqbal 

00966544639978 (whatsapp) 

Kannayeram Gnanapandithan

unread,
Aug 9, 2022, 8:39:58 AM8/9/22
to materials-welding
preheat minimum-- Ambient >_15°C.   Interpass max-- 155°C

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP9k9Xfi4e1V_EZ4T04hQ-uKT4W6G-k6iYrnY0Jh%3D0_pKXsAog%40mail.gmail.com.

Dragan Mancic

unread,
Aug 10, 2022, 10:24:41 AM8/10/22
to material...@googlegroups.com
Reply all
Reply to author
Forward
0 new messages