Dear Expert
we have hot tapping 
from process piping b31.3 design 
to cross country pipeline old pipe i think api 1104 design
WPS that need to folow  api 1104 or asme b31.3.
best regard.

K.M Hrishikesan

unread,
Feb 24, 2025, 4:01:17 AM2/24/25
to material...@googlegroups.com
Hi

You have to follow API 1104 Annex B for qualifying the procedure

Regards
Hrishikesan

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/ffa0c881-23d8-4b3f-96d1-7337ed4ac1e1n%40googlegroups.com.

Luis Opazo Zenteno

unread,
Feb 27, 2025, 11:58:14 PM2/27/25
to ali owead, Materials & Welding
Definitely, to qualify the procedure, you must follow API 1104 Annex B.
And by the way, our experience in hot tap fitting welding projects, on pipelines with gas flow, API 5L X60 pipe, Ø 12" and API 5L X70 pipe, Ø 16".

best regard
Luis Opazo Z.
+56 9 983 370 40.

De: material...@googlegroups.com <material...@googlegroups.com> en nombre de ali owead <alia...@gmail.com>
Enviado: lunes, 24 de febrero de 2025 6:38
Para: Materials & Welding <material...@googlegroups.com>
Asunto: [MW:35448] Hot tapping between piping and pipeline
 
--

Sudhakar Kuppuswamy

unread,
Feb 28, 2025, 10:46:17 PM2/28/25
to material...@googlegroups.com
Hello,  

ASME B31.3 is not having any references clause for HOT welding procedure qualifications. 

Yes, the fitting design shall be designed inline to B31.3 for process piping and the field welding of the fitting on the live system shall be done as per API 1104 . 

Note : In case of fitting fabrication, let say in barred tee the weld joint between flange and sleeve , the shop welding can be carried out inline to ASME section IX. 

Regards,

Sudhakar K CEng MWeldI,IWE.

Welding & Metallurgical Engineer,

Email: sudhak...@gmail.com.



--