JIS G 3115 SPV 490 Q in welding requirement
Hi everybody
Can you support me some information for JIS G 3115 SPV 490 Q in welding requirements with thickness over 24 mm in sphere tank according to ASME VIII Div.2:
- Preheat
- Post weld heat treatment
- Hardness testing requirement for PQR
Thank you & Best regards
TRAN VAN VUONG
--
To post to this group, send email to
material...@googlegroups.com
To unsubscribe from this group, send email
to materials-weld...@googlegroups.com
For more options, visit
this group's bolg at http://materials-welding.blogspot.com/
The
views expressed/exchnaged in this group are members personel views and meant for
educational purposes only, Users must take their own decisions w.r.t. applicable
code/standard/contract documents.
THIS MESSAGE IS ONLY INTENDED FOR THE USE OF THE INTENDED RECIPIENT(S) AND MAY CONTAIN INFORMATION THAT IS PRIVILEGED, PROPRIETARY AND/OR CONFIDENTIAL. If you are not the intended recipient, you are hereby notified that any review, retransmission, dissemination, distribution, copying, conversion to hard copy or other use of this communication is strictly prohibited. If you are not the intended recipient and have received this message in error, please notify me by return e-mail and delete this message from your system. Ontario Power Generation Inc.