Dear All
We have encountered a critical issue with the joints from the beam to the main plate on the Spud Can top plate of our jack-up rig. Upon welding and subsequently lowering the spud can into the water using the jacking system, cracks have emerged in three of the joints that were welded previously ( according to photos cracks happen on the plate) This is a concerning development, and we must address it promptly to ensure the integrity and safety of our spud can.
Considering that in the area where we are, the depth of water is low and there is not much pressure on the spud can, the reason why this happens is not clear to us, and if anyone can advise on this matter, I would be very grateful.

Main top plate thickness is 19 mm and crack depth is 16 mm.

Regards
Babak

WhatsApp Image 2024-03-29 at 8.04.41 PM (1).jpeg
WhatsApp Image 2024-03-29 at 8.04.38 PM (1).jpeg

Ramamoorthi Thangarasu

unread,
Mar 31, 2024, 10:22:14 AMMar 31
to material...@googlegroups.com
Hi 

This same problem we have solved in my previous Project .  It's called Hydrogen induced Crack or Delayed Crack. The main reason WPS was not followed (Preheating and post heat ) .   Also need to check two times for NDT 24 hours and 48 hours.   

Regards
Ramamoorthi Thangarasu
Sr.Inspection Engineer
TUV Rheinland.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1896576593.3616147.1711818946138%40mail.yahoo.com.

Manoj Singh

unread,
Apr 1, 2024, 12:50:41 AMApr 1
to material...@googlegroups.com
Please check for CEV value as we have also experienced the same type of crack and we found CEV was higher than max required.

Regards

Vinay

unread,
Apr 1, 2024, 12:50:42 AMApr 1
to material...@googlegroups.com
Dear ;

Can you please provide more details ... MOC ?? ,Welding process ?? Preheat /Post heat??

Venkatesh Mech

unread,
Apr 1, 2024, 10:35:04 AMApr 1
to material...@googlegroups.com
Hello sir, 

We are also faced similar issue. Now is it possible to rework the part.

CHITTARANJAN BHIWANDKAR

unread,
Apr 1, 2024, 10:35:09 AMApr 1
to material...@googlegroups.com
Are these cracks on plates near the leg joint.
Where "D" class plates are used.

Mostafa DAIF

unread,
Apr 1, 2024, 12:02:47 PMApr 1
to material...@googlegroups.com
Dear all,

What is the material specification of the plate?

Best Regards,



--

Mostafa DAIF
Chef preparateur

T : 05 23 38 90 72
M : 06 61 54 12 95
TAQA MOROCCO PB 99 Sidi Bouzid - El Jadida 24 000 - Maroc
taqamorocco.ma

TAQA MOROCCO is a member of the Abu Dhabi National Energy Company Group of companies.
  

The information contained in this communication is confidential, may be attorney-client privileged, and is intended only for the use of the addressee. It is the property of Abu Dhabi National Energy Company PJSC (TAQA) or one of its affiliates. Unauthorized use, disclosure or copying of this communication or any part thereof is strictly prohibited and may be unlawful. If you have received this communication in error, please notify me immediately by return email and destroy this communication and all copies thereof, including attachments.


Reply all
Reply to author
Forward
0 new messages