Is PWHT required

105 views
Skip to first unread message

Nadakuditi kiran kumar

unread,
Oct 2, 2019, 1:06:12 AM10/2/19
to material...@googlegroups.com
Dear Gentleman,
We have received two vessels as per drawing. ASME U stamp done on both vessels, there is one bottom outlet nozzle of 6"NB in both vessels. Now client is asking us to remove the flange of the nozzle and hook up with piping. My doubt is 
1. Whether we have to take approval from authorized inspector before going to do any modification.
2. After hook up we have to do PWHT for that hook up joint
Please clarify, if possible please provide code reference.
Line SERVICE not call any PWHT
Construction code for vessel is ASME Sec VIII, Div 1, piping construction code is B 31.3.

Thanks in advance,


Hemant W Joshi

unread,
Oct 3, 2019, 4:30:07 AM10/3/19
to material...@googlegroups.com

Without knowing the piping matl or thickness, it would be imprudent to provide opinion about PWHT.

The flange it is assumed is a SO.  

Certainly it is required to communicate to the inspector for reinspection/restamping.   

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABQUuFiLcCT5%3DUCLMF4C013RpSb2mPfFMRwcBhLGL%3Dzq21ca_w%40mail.gmail.com.

---------------------------------------------------------------------------------------------------------- Information transmitted by this E-MAIL is intended only for the use of the addressee(s) and contains information that is privileged, confidential or exempt from disclosure under applicable law. If you are not the intended recipient or it appears that this mail has been forwarded to you without proper authority, you are notified that any use or dissemination and or copying of this email in any manner is strictly prohibited and you are requested to delete this e-mail immediately. Communicating through e-mail is not secure and capable of interception and delays. Any one communicating with TATA Consulting Engineers Ltd., and / or its subsidiaries or associates or group companies by e-mail accepts the risks involved and their consequences. While this e-mail has been checked for all known viruses, the addressee should also scan for viruses and notify the originator of e-mail. ---------------------------------------------------------------------------------------------------------

José Juan Jiménez Alejandro

unread,
Oct 3, 2019, 4:30:08 AM10/3/19
to material...@googlegroups.com
Greetings !, I see that it is a modification or alteration, usually this type of work is stamped "R" of the NB, I suggest you speak it with your Authorized Inspector that you have assigned to your company (this in case your company is certified with ASME and NB), as for the PWHT depends on the number P of the material and its thickness, consult it with your ASME Inspector.
Regards!.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABQUuFiLcCT5%3DUCLMF4C013RpSb2mPfFMRwcBhLGL%3Dzq21ca_w%40mail.gmail.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





Rishikesh Kumar

unread,
Oct 3, 2019, 6:07:07 AM10/3/19
to material...@googlegroups.com
it is advice to do any modification or alteration with proper procedure.  this procedure shall be required approval from client / nominated TPI. PWHT depends on various parameters line P. No./ Group No. /thickness/ Pressure part/No Pressure parts etc  UCS -56 is refer for the same for decide PWHT required. 
for eg: for carbon steel grade material UCS-56-1 is applied. further there is provision provided to perform welding with preheating upto thickness 38mm ( general note a) and b)) without preheating. the similar provision is also incorporated in latest edition of B31.3 
Regards
Rishikesh kumar 

Nadakuditi kiran kumar

unread,
Oct 3, 2019, 7:42:39 AM10/3/19
to material...@googlegroups.com
dear gents,
Please find below mentioned details.
MOC is A333 Gr 6, thickness of nozzle is 6" NB-14.27mm, pipe thickness is 6" NB -7.11 mm. Flange is WNRF - A350 LF2{(Which needed to be cut).


Hemant W Joshi

unread,
Oct 4, 2019, 6:03:34 AM10/4/19
to material...@googlegroups.com

Considering that A333 gr.6 is P-1 , there appears to be no PWHT requirement as per 31.3 table 331.1.1purely for the butt weld joint between the pipe portion of nozzle and the piping to be hooked up with it considering the pipe thickness .

 

It would be better if the specification writeup is shared to understand as to why PWHT has been put in place for the piping concerned as per your statement.  

Rishikesh Kumar

unread,
Oct 4, 2019, 6:34:23 AM10/4/19
to material...@googlegroups.com
Since both the material are  P No. 1.  it may proceed since  this alteration is required from your end. However,  proper procedure  from Initial stage ( removal) to final stage (NDT) should be  informed  and get approval if required and recorded for future reference.
further, please make sure,  welding shall be  performed with established WPS and qualified Welder.
Regards
Rishikesh kumar

CLV

unread,
Oct 6, 2019, 11:40:19 PM10/6/19
to Materials & Welding
As suggested by Jose the modification must be under R stamp,if u hv completed MDR & registered with NB.
Modification is possible as per customers requirements.Also PWHT after modifications may not be required if WPS/PQR is available.
Reply all