Please advice whether for SA105 material, fully killed steel is required to be mentioned in the MTC.

Thanks & Regards,

Anthony.C

George Dilintas

unread,
Aug 6, 2016, 6:11:42 AM8/6/16
to Meghanadh K
SA-961 which is the basic spec for forgings specifies in para. 5 that steel must be fully killed. So since SA-105 makes reference to SA-961, the steel for SA-105 has to be fully killed. However, both standards do not require to have this info on the MTR

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/80e09b87-8f5f-47a8-8b52-ce20f584a674%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
Reply all
Reply to author
Forward
0 new messages