Radiography can be done After Hydrotest

425 views
Skip to first unread message

pradip kumar Sil

unread,
May 9, 2020, 1:12:23 AM5/9/20
to materials-welding
Dear All,
 Radiography  can be done after Hydrotest. What's the limitation of  ASME B-31.3.
Before Hydrotest all Radiography can be completed. ASME -B-31.3 Code reference ?
Your advice is highly appreciated with code reference ASME B-31.3.
Regards,
Pradip

SENTHILKUMAR SWAMINATHAN

unread,
May 9, 2020, 1:37:25 AM5/9/20
to material...@googlegroups.com
Yes, you can do. provided your graphs should have within limited indications as per acceptance table. 
In case any one weld goes repair hydro test shall be done. 
Regards, 
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8%3DwM9yo%2B%3DLuNU3J185gWHOmY5DHvxnpvLz_uF3BVnjkUg%40mail.gmail.com.

atul khatri

unread,
May 11, 2020, 12:59:10 AM5/11/20
to material...@googlegroups.com
As per ASME B 31.3 ,clause 345  "Prior to initial operation, and after completion of the applicable examinations required by para. 341, each piping system shall be tested to ensure tightness. The test
shall be a hydrostatic leak test in accordance with para. 345.4 except as provided herein."
Here clause 341 calls for NDT and Visual examination. 
Hope its clear now that hydrotest shall be after NDT but if client accepts than sequence can be reversed.

Thanks and regards
Atul Khatri

Mohamed Mujahith

unread,
May 11, 2020, 2:24:35 AM5/11/20
to material...@googlegroups.com
as per ASME 31.3 , we are completed RT repair next move hydro test what my question "how to start the leak test process what kind of document i submitted to client then should be arrange water lab test report to through client , further i need for reference of diagram , procedure and test report sample document.' so please anybody provided your copy for guidelines and help me.
hope to your highly response and awaiting reply.........

   @thoufi...@gmail.com for your information follow ASAP

thanks and regards
Mohamed Mujahith