Dear Friends,

Please can you advise in which EIL Standard or API standard  to find the material certification requirement  EN3.1 or 3.2 or 2.2 for Pumps ( various components) in EIL Specification.

waiting for your response.

thanks.
Ahmed

Dinesh Somwanshi

unread,
Dec 19, 2018, 8:34:01 AM12/19/18
to materials-welding
Dear sir,

EN 3.1 MTC components  Certification basically based on review of test results.
EN 3.2 MTC components Certification basically based on witness of test results.  

Thanks & Regards

DINESH VITTHAL SOMWANSHI

BACHELOR IN MECHANICAL ENGINEER

AUTHORIZED PIPING / WELDING / NDT / PAINTING INSPECTION PERSONNEL
API 570 - Piping Inspector, AWS - CWI , CSWIP 3.1*,*BGAS  Gr 2 / 3
NDT II -UT , RT , MT , PT, VT
 00919881344135 India 
Skype = dinesh somwanshi

असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Perumal Govindan

unread,
Dec 19, 2018, 8:42:49 AM12/19/18
to material...@googlegroups.com

Please refer BSEN 10204 for.more information

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

shaikh ahmed

unread,
Dec 19, 2018, 10:51:18 PM12/19/18
to material...@googlegroups.com
Dear Experts,

Material Certification for PUMP components as per EIL Standard or API Standard  ( whether it is EN10204-3.1 / 3.2/2.2 for Pump components)

Please can you advise in which EIL Standard or API standard  to find the material certification requirement for Pump whether it is require   EN3.1 or 3.2 or 2.2 for Pumps various components in EIL Specification or API Standard

Perumal Govindan

unread,
Dec 19, 2018, 11:11:49 PM12/19/18
to material...@googlegroups.com

Hi
Based on the criticality rating of the equipment's, the material certification requirements are decided.

Refer the pump MR (Maternal Specification), project purchase material specification / pump data sheet, there you can get the complete information.

Regards
P Govindan

Perumal Govindan

unread,
Dec 19, 2018, 11:36:30 PM12/19/18
to material...@googlegroups.com

Hi

2.2 certification is a certificate contains  compliance of a product (COC) or un tested data of a product.

3.1 certification is a certificate contains the physical and chemical properties / performance tests are  tested at manufacturer laboratory or outside accredited laboratory and the tests are witnessed by the quality department of the manufacturer. Simple we can call as a manufacturer quality certificate.

3.2 certificate is a certificate contains all the physical & chemical properties / all the performance tests/FAT (Factory Acceptance Tests) are witnessed by both quality department personnel of the manufacturer and third party inspection agency's Inspector.

I hope above information clear about the certification levels.

Regards
P Govindan

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

israr

unread,
Oct 8, 2024, 5:04:35 AM10/8/24
to Materials & Welding
Hi 
Can any body respond at what stage an independent inspector witness material testing for certification of 3.2.?

shaikh ahmed

unread,
Oct 8, 2024, 6:43:16 AM10/8/24
to material...@googlegroups.com
For Valve case it should be from Pouring to final test 
For Plate/Pipe- start from Raw material to final test

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f794a65b-0632-4fe1-b9e0-7ed4a33c9c5an%40googlegroups.com.

israr

unread,
Dec 27, 2024, 7:29:40 AM12/27/24
to Materials & Welding
Dear Perumal,
I answer the same but got one more question where it is written that TPI witness is mandatory?


israr

unread,
Dec 27, 2024, 7:29:48 AM12/27/24
to Materials & Welding
Hi Team,
Can anybody tell How TPI certify material for 3.2 certification?
Is realy witness required? if Required @ which stage?

Raghuram Bathula

unread,
Dec 27, 2024, 7:32:14 AM12/27/24
to Materials-Welding
Refer BS EN 10204, note TPI from purchaser

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Sankaran Sp

unread,
Dec 28, 2024, 12:05:25 PM12/28/24
to Materials & Welding
Dear friend,

EN 10204 3.1 - means - manufacturers issuing certifcate with chemical, mechnical test result by signing Quality engineer & qulaity manager 
EN 10204- 3.2 - means -  Third party agency issuing a certifcate after witnessing the chemical, mechnical test result at manaufacturer place or common lab and signing TPI witnessing  engineer with support of raw materail test certicate with heat number traceabilty.      

Regards,
Sankaran.SP
Welding & Metallurgy expert
Coimbatore, India. 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com

suhel....@gmail.com

unread,
Dec 31, 2024, 10:28:40 PM12/31/24
to Materials & Welding
The definition of 3.2 certification as per EN 10204 is : 

Document prepared by both the manufacturer’s authorized inspection representative, independent of the manufacturing department and either the purchaser's authorized inspection representative or the inspector designated by the official regulations and in which they declare that the products supplied are in compliance with the requirements of the order and in which test results are supplied