Is flush grinding of welds acceptable in pressurevessels or pipes. If so please let me know the ASME code clause or some code reference.
Thanks & Regards
Gurunath Hanamar
Dear Guru,Grinding the welds is permitted to the extent that at no place should the weld metal "fall below the surface of the adjoining base materials" -- see UW 35 (d). Proving that may be a difficult job, hence always leave a reinforcement unless constrained by design.RegardsBM
--