Welding Symbol

82 views
Skip to first unread message

vikas shelke

unread,
Mar 11, 2012, 8:09:46 AM3/11/12
to material...@googlegroups.com
Inline image 1

Please tell meaning of the "141" in welding Symbol.

 
 Regards,
 
Vikas Shelke,


image.png

Karthik

unread,
Mar 11, 2012, 10:42:47 PM3/11/12
to material...@googlegroups.com
Its an European Standard Symbol.
141 - GTAW 
111-SMAW
121-SAW
135-GMAW
136-FCAW
 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
German-Thai Boiler Engineering Cooperation Limited.
Rayong Factory ;
379 Moo.6 Soi 8, Tambol Pananikom,
Nikompattana, Rayong 21180 THAILAND
Tel : +66 38 897 035-9 Ext. 137
Hand Phone: 0066 892512282


From: vikas shelke <vikas.s...@gmail.com>
To: material...@googlegroups.com
Sent: Sunday, March 11, 2012 7:09 PM
Subject: [MW:13860] Welding Symbol

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


image.png

K.Babu

unread,
Mar 11, 2012, 10:38:55 PM3/11/12
to material...@googlegroups.com
141- DNV-0S-C401 --------GTAW Process
 


 

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & regards,

K.Babu
image.png

rajkumarantoni

unread,
Mar 11, 2012, 11:10:13 PM3/11/12
to material...@googlegroups.com

I have not seen with traingle symbol,it's very odd

image.png

Sanu Krishnan

unread,
Mar 11, 2012, 10:52:34 PM3/11/12
to material...@googlegroups.com
Vikas,

 141 represents the welding process ,As per BN 4063:2000- Numerical indications of selected welding process

141- Tig welding




--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks and regards
 
SANU.K.NAIR
QC INSPECTOR
Ph: 0507464738
 
         "Try to be a man with values".                               
 
   It's Possible
  ABUDHABI
 

image003.jpg
image.png

Kavin Murugam

unread,
Mar 12, 2012, 2:10:30 AM3/12/12
to material...@googlegroups.com

As per requested,
 
Kavin Murugam
0126159644
welding reff no.JPG