Hi friend,
Pls check it once, HT pressure will be 1.5 times of working pressure, or 95% of the design pressure, but not 1.5 times of the design pressure…
Understand the concept …. (it might be a pipe line, or a vessel)
1. Working pressure is defined for which the system is to be worked (ex. 100BAR)
2. Design pressure is defined for which the system is defined, it is always higher than working pressure to ensure safety and considering all the constructional stress i.e we can say 1.5 times of working (it will be 150BAR, in the above case)
3. Hydro test pressure – should be above working and below to the designed – as your system is designed for 150BAR – you cannot test it for 1.5 times of the design pressure say 225 BAR, test pressure will be always less than 150bar to ensure system safety. or else in extreme case you can go up to 150 Bar – 100% of the design pressure – but not more than that
Thanks & Regards,
Lakshman Kumar B,
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2Bk3Rc_mjMokD%2B_%3Dc5sDUHMHicaqRJTZ19xWE1ZPAxARxLFYaQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Dear friend,
Please provide basis for trailing email quote.
General assumption is not applicable for such a hydro test pressure.
Regards,
Vijay
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2Bk3Rc_mjMokD%2B_%3Dc5sDUHMHicaqRJTZ19xWE1ZPAxARxLFYaQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/003201d20b1f%242b2962f0%24817c28d0%24%40gmail.com.
Please let us know complete details,
Which code of construction?
Service?
Client spec?
Any special considerations?
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2Bk3Rc_mjMokD%2B_%3Dc5sDUHMHicaqRJTZ19xWE1ZPAxARxLFYaQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/003201d20b1f%242b2962f0%24817c28d0%24%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPi2c29sJxJsC83tPOpqZa1-Yz_%3DF3wO7P0ux26%3DOZAPUR-AUQ%40mail.gmail.com.
For hydro test pressure please refer UG99 b of ASME Sec. VIII Div. 1.
Generali MAWP is designe pressure.
Regards.,
Prasad G.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2Bk3Rc_mjMokD%2B_%3Dc5sDUHMHicaqRJTZ19xWE1ZPAxARxLFYaQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/003201d20b1f%242b2962f0%24817c28d0%24%40gmail.com.
Prasad Rode
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2Bk3Rc_mjMokD%2B_%3Dc5sDUHMHicaqRJTZ19xWE1ZPAxARxLFYaQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.