What Is Carbon Steel A105 Grade 2

2,086 views
Skip to first unread message

Jatin Sanghvi

unread,
Oct 24, 2013, 1:37:47 AM10/24/13
to material...@googlegroups.com
Dear Expert,

A client of mine has specified Class 150 carbon steel flanges as per ASTM A105 Grade 2. Does anyone know the composition and material characteristics of "Grade 2". I do not see any reference to Grade 2 in the latest (2010) version of ASTM A105 standard.

Any reference to direction would be most appreciated.

Best Regards
Jatin Sanghvi
Mobile: 0091-9823458877

John Henning

unread,
Oct 24, 2013, 10:33:35 AM10/24/13
to material...@googlegroups.com

A/SA-105 does not have any class or grade break down.  However, A/SA-105 references A/SA-266, Specification for Carbon Steel Forgings for Pressure Vessel Components, which has four grades.  You would have to enquire from your client, but I think it is possible that the intent was for the forgings to meet 266 grade 2 properties.

 

John A. Henning

Welding & Materials

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

Tahir Olmez

unread,
Oct 24, 2013, 4:47:03 PM10/24/13
to material...@googlegroups.com
Dear friend , grade 2 mentions the tensile strench pls check the link for furthrt info http://www.turnkeyips.com/assets/astm_specifications_for_weld_fittings_and_flanges.pdf
Tahir Bilge Ölmez
International Welding engineer