Re: [MW:23413] Procedure Qualification Hot wire vs Cold wire TIG

74 views
Skip to first unread message

Raghuram Bathula

unread,
Sep 7, 2015, 5:46:51 AM9/7/15
to Materials-Welding
is Impact testing required? it will effect other parameters, for e.g QW 409.1 (travel speed and amp are higher in case of hot wire)

On 7 September 2015 at 13:25, FAIRON Luc <luc.f...@cmigroupe.com> wrote:

I have got a PQR qualified for orbital TIG welding (automatic) with cold wire. Does it qualify for orbital TIG welding with hot wire, all other thinks remaining unchanged ? In my opinion yes, but I am not sure. Applicable construction code is ASME. Welding qualifications are per Section IX.

Regards

 

Luc FAIRON
Welding Engineer

 

 


FAIRON Luc

unread,
Sep 7, 2015, 5:59:13 AM9/7/15
to material...@googlegroups.com

Base material is stainless steel and there is no impact requirement (no supplementary essential variable)

 

Luc Fairon

 

De : material...@googlegroups.com [mailto:material...@googlegroups.com] De la part de Raghuram Bathula
Envoyé : lundi 7 septembre 2015 11:46
À : Materials-Welding
Objet : Re: [MW:23414] Procedure Qualification Hot wire vs Cold wire TIG

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubk7YYMvF3GiWQ96OdiLqWN_yRGemiCgATEiwtJGf2hDoQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.




CONFIDENTIALITY NOTICE:
The information in this communication and any attachments is intended only for the use of the addressee and may contain information that is privileged, business sensitive, strictly private, confidential or otherwise protected from disclosure. If you, reader of this notice, are not the intended recipient, you are hereby notified that any use, dissemination, distribution, or copying of this communication is strictly prohibited. If you have received this communication in error, please notify the sender and delete the communication without retaining any copies.

Raghuram Bathula

unread,
Sep 7, 2015, 6:28:53 AM9/7/15
to Materials-Welding
yes , you can
Pl. refer attachment 
tip-tig-weld-qualification.pdf