Distance between two L-Seam

5,739 views
Skip to first unread message

Gurunath.Hanamar

unread,
Jun 13, 2012, 11:24:41 PM6/13/12
to material...@googlegroups.com

Dear all,
I know that 100mm is permissble distance between two consecutive longitudinal seams but, can any one confirm minimum distance between two longitudinal seams should be mantained. Kindly mention ASME clause.

Thanks &Regards
Gurunath Hanamar

george....@gr.bureauveritas.com

unread,
Jun 14, 2012, 2:50:19 AM6/14/12
to material...@googlegroups.com

Section VIII-1 UW(9)(d): except when the longitudinal joints are radiographed 100 mm each side of each circumferential welded intersection, vessels made up of two or more courses shall have the centers of the welded longitudinal joints of adjacent courses staggered or separated by a distance of at least five times the thickness of the thicker plate


best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor
API 510 Inspector

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04

Inactive hide details for "Gurunath.Hanamar" <guru.h10@gmail.com>"Gurunath.Hanamar" <guru...@gmail.com>



To


cc


Subject

    [MW:14538] Distance between two L-Seam

Ref

Thanks &Regards
Gurunath Hanamar

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
NOTICE: This message contains information which is confidential and the copyright of our company or a third party. If you are not the intended recipient of this message please delete it and destroy all copies. If you
are the intended recipient of this message you should not disclose or distribute this message to third parties without the consent of our company. Our company does not represent, warrant and/or guarantee that the integrity of this message has been maintained nor that the communication is free of virus, interception or interference. The liability of our company is limited by our General Conditions of Services.
Nota : Ce message contient des informations confidentielles propriété de notre société et/ou d'un tiers. Si vous n’êtes pas parmi les destinataires désignés de ce message, merci de l'effacer ainsi que toutes ses copies. Si vous êtes parmi les destinataires désignés de ce message, prière de ne pas le divulguer ni de le transmettre à des tiers sans l’accord de notre société. Notre société ne peut garantir que l’intégrité de ce message a été préservée ni que la présente communication est sans virus, interception ou interférence. La responsabilité de notre société est limitée par nos Conditions Générales de Services.
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~

suresh kumar

unread,
Jun 14, 2012, 3:22:14 AM6/14/12
to material...@googlegroups.com, guru...@gmail.com


Dear guru,

I am also asked this question to all of our friends, still no body can answer for this ...because as per ASME there is no answer available, but in my project specification(SGD- ABUDHABI) 150 mm is allowed..

..

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
*T.SURESHKUMAR. B.E, M.B.A, NDT LEVE-II.,
QA/QC INSPECTOR (PIPING, WELDING,STRUCTURAL)
DODSAL ENGINEERING & CONSTRUCTION PTE LTD,
ABUDHABI,
UAE.
*
*
*









Saravanan Sornam

unread,
Jun 14, 2012, 3:56:49 AM6/14/12
to material...@googlegroups.com
Hi Guru,
 
You can find in ASME VIII Div. I, UW-9 (d).
 
(d) Except when the longitudinal joints are radiographed
4 in. (100 mm) each side of each circumferential welded

intersection, vessels made up of two or more courses shall
have the centers of the welded longitudinal joints of adjacent
courses staggered or separated by a distance of at
least five times the thickness of the thicker plate.
 
Hope it is Ok for U...
 
Cheers,
Sarav,
Korea

--

Gurunath.Hanamar

unread,
Mar 28, 2013, 7:17:35 AM3/28/13
to material...@googlegroups.com
Dear Mr. Himanshu,

As per B 31.3 seam to seam minimum distance is given as 4 times thickness but B 31.3  haven't mentioned L seam to L seam staggering. Means can be weld without staggering.

ವಂದನೆಗಳೊಂದಿಗೆ / Best regards, 
Gurunath Hanamar


On Thu, Mar 28, 2013 at 11:11 AM, Himanshu Patel <absg...@gmail.com> wrote:
Hello To ALL,
 
This clause applicable to Pressure Vessel, What about PIPING can any one suggest for piping as per (API 1104, B31.4, B31.3 or B31.1).
 
Thanks.

 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

Nandesh Kumar

unread,
Mar 28, 2013, 5:11:04 PM3/28/13
to material...@googlegroups.com
Such stuff are referenced in corresponding project specifications, as these can not be generalised.

ವಂದನೆಗಳೊಂದಿಗೆ / Best regards,

Nandesh Kumar A

Abu Dhabi, UAE

P.S. : Please don't print this e-mail unless you really need to.


--- On Thu, 28/3/13, Himanshu Patel <absg...@gmail.com> wrote:

Ritixa Tandel

unread,
Mar 21, 2016, 6:27:29 AM3/21/16
to Materials & Welding
HELLO,

I AM STUDYING & REFERRING ABOUT DESIGN OF EQUIPMENT. 

CONTINUE TO YOUR DISCUSSION ABOUT ''DISTANCE BETWEEN TWO L-SEAM''........

WHAT SHOULD BE THE MINIMUM DISTANCE IF MY REACTOR IS LIKE THIS:

--SS 316 L REACTOR (3 KL WORKING CAPACITY)
--SHELL: 1500 MM ID x 1700 MM LG x 8 MM THK
--REACTOR WITH DOUBLE LIMPET COIL.

REGARDS RITIXA.
ANKLESHWAR, GUJARAT. INDIA.

dili...@gmail.com

unread,
Apr 1, 2016, 12:46:50 AM4/1/16
to Materials & Welding
ASME Code has a restrictions for staggering. You may use this one

Sent from my BlackBerry 10 smartphone.
From: Ritixa Tandel
Sent: Δευτέρα, 21 Μαρτίου 2016 - 12:27
To: Materials & Welding
Subject: Re: [MW:24562] Distance between two L-Seam


The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Kannayeram Gnanapandithan

unread,
Apr 1, 2016, 2:03:02 AM4/1/16
to materials-welding
check in sec 8, think 5Xthick mm 

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

Krunal Gajjar

unread,
Apr 18, 2018, 8:11:10 AM4/18/18
to Materials & Welding
WHY DISTANCE REQUIRED??

KRUNAL

udaya bhaskar

unread,
Apr 19, 2018, 12:04:57 AM4/19/18
to material...@googlegroups.com
My dear, distance between two L seams for pressure vessels minimum 250- 300mm.

On Mon 21 Mar, 2016, 15:57 Ritixa Tandel, <ritixat...@gmail.com> wrote:
HELLO,

I AM STUDYING & REFERRING ABOUT DESIGN OF EQUIPMENT. 

CONTINUE TO YOUR DISCUSSION ABOUT ''DISTANCE BETWEEN TWO L-SEAM''........

WHAT SHOULD BE THE MINIMUM DISTANCE IF MY REACTOR IS LIKE THIS:

--SS 316 L REACTOR (3 KL WORKING CAPACITY)
--SHELL: 1500 MM ID x 1700 MM LG x 8 MM THK
--REACTOR WITH DOUBLE LIMPET COIL.

REGARDS RITIXA.
ANKLESHWAR, GUJARAT. INDIA.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Rajesh Kasvala

unread,
Apr 19, 2018, 12:11:01 AM4/19/18
to material...@googlegroups.com
Pl refer uw9 D



---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

tugrulhan özdemir

unread,
Apr 20, 2018, 6:00:16 AM4/20/18
to material...@googlegroups.com
Storage tanks has limitation like below in API 650:

 "Vertical  joints  in  adjacent  shell  courses  shall  not  be  aligned,  but  shall  be  offset  from  each  other  a  minimum
distance of 5t, where t is the plate thickness of the thicker course at the point of offset. "     

which is not applicable in real since results flat spots.



Also

EN 13445-4:2009

6.2 Vessels or parts made of more than one course

Where a vessel or vessel part is made of two or more courses the longitudinal weld joints of adjacent courses shall be staggered by 4 e with 10 mm minimum, or 30 mm minimum when the vessel or vessel part is either working in the creep range or designed by Design by Analysis – Direct Route (Annex B of EN 13445-3:2009) or designed using 6.3 of EN 13445-3:2009.




2018-04-19 7:10 GMT+03:00 'Rajesh Kasvala' via Materials & Welding <material...@googlegroups.com>:
On Thu, Apr 19, 2018 at 9:34 AM, udaya bhaskar
My dear, distance between two L seams for pressure vessels minimum 250- 300mm.

On Mon 21 Mar, 2016, 15:57 Ritixa Tandel, <ritixat...@gmail.com> wrote:
HELLO,

I AM STUDYING & REFERRING ABOUT DESIGN OF EQUIPMENT. 

CONTINUE TO YOUR DISCUSSION ABOUT ''DISTANCE BETWEEN TWO L-SEAM''........

WHAT SHOULD BE THE MINIMUM DISTANCE IF MY REACTOR IS LIKE THIS:

--SS 316 L REACTOR (3 KL WORKING CAPACITY)
--SHELL: 1500 MM ID x 1700 MM LG x 8 MM THK
--REACTOR WITH DOUBLE LIMPET COIL.

REGARDS RITIXA.
ANKLESHWAR, GUJARAT. INDIA.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.



--

Saygılarımla / Regards


Tuğrulhan ÖZDEMİR

API 653 AI, Welding & Materials Eng.

ASNT VT, PT, MT, RT L-II

+90 539 747 2676


Dindo

unread,
Apr 20, 2018, 10:31:36 PM4/20/18
to material...@googlegroups.com
ASME Sect VIII Div 1 2017 Ed.: UW-9(d)

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

Souravbohray

unread,
Oct 10, 2018, 10:19:43 PM10/10/18
to Materials & Welding
When the vessel is 100% RT than long seam can be at same line ? 100 radiographed on each c seam is consider when RT for vessel is spot? So it's mean when spot RT is there in vessel than only we have to maintain 5 T criteria for long seam setup.because ASME code use word "EXCEPT "- means remains the other.