ASME SEC VIII Div1- UG-36 & UG-42 Nozzles RF pad requirements & mulitiple Nozzles opening

1,305 views
Skip to first unread message

Ponnikumar

unread,
Apr 29, 2024, 9:25:53 AM4/29/24
to material...@googlegroups.com
Dear all,
Kindly refer to the attached images of the 
2 instrument air vessels.
one vessel 6" nozzles with reinforcement pad and other one same 6" nozzles without RF pad. Top head diameter, design pressure, head thickness , nozzle to head weld is internal portrusion with back side welding also same

From UG-36 above 10mm thickness only 2.3/8" ID nozzles can fabricate with out reinforcement pad.

Queries:
1. 6" nozzles required RF pad or not? With details explain 
2. 6" nozzles in-between 2" nozzles with maintain 500mm centre to distance - min distance requirements.


D5511C V1 photo1.jpg
D5511A V1 photo.3png.jpg
D5511C V1 photo.4.jpg
D5511A V1 photo.7.png
D5511A V1 photo1.png

Amol Betkar

unread,
Apr 29, 2024, 11:41:06 PM4/29/24
to material...@googlegroups.com

Dear,

Let's address each query with detail:

  1. 6" nozzles required RF pad or not? According to the ASME Boiler and Pressure Vessel Code, Section VIII, Division 1, specifically in UG-36, when the thickness of the vessel wall exceeds 10 mm (or 0.394 inches), reinforcement pads are typically required for nozzles larger than 2 3/8" ID. However, there are exceptions based on specific design considerations and loadings.

    In the case of the vessels you mentioned, if the thickness of the vessel wall where the 6" nozzles are located exceeds 10 mm, then RF pads may be required. The decision to use RF pads depends on factors such as the design pressure, vessel material, service conditions, and nozzle loads. RF pads help distribute the stresses and loads at the nozzle-to-vessel junction, enhancing the structural integrity of the vessel.

    Engineers and fabricators need to conduct detailed stress analysis and consider factors like nozzle loads, internal and external pressures, thermal effects, and the mechanical properties of the vessel material to determine whether RF pads are necessary. Additionally, industry standards and codes may provide further guidance specific to the application.

  2. 6" nozzles in-between 2" nozzles with maintaining 500mm center-to-center distance - minimum distance requirements: Maintaining adequate spacing between nozzles is crucial to ensure proper operation, maintenance access, and structural integrity of the vessel. The minimum distance between two nozzles depends on various factors, including vessel design, nozzle size, nozzle type, and applicable codes and standards.

    In the scenario you described, where 6" nozzles are positioned between 2" nozzles with a specified center-to-center distance of 500 mm, it's essential to confirm whether this distance meets the minimum requirements outlined in the relevant design codes and standards, such as ASME BPVC Section VIII, Division 1.

    Typically, the minimum distance between two nozzles is determined to prevent interference, facilitate maintenance activities, and ensure proper reinforcement of the vessel walls around each nozzle. Factors such as the diameter and orientation of the nozzles, nozzle loads, and vessel geometry influence the minimum spacing requirements.

    Engineers and designers should refer to the applicable design codes, conduct stress analyses, and consider specific project requirements to determine the suitable spacing between the 6" and 2" nozzles. If the specified center-to-center distance of 500 mm meets or exceeds the minimum requirements specified in the applicable codes and standards, it should be acceptable. However, it's crucial to verify this through thorough engineering analysis and review.

Regards,

Amol K.B

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKL%3DdYwuPbWBjMbyfZcbS4De_tJ23EVbs4KSNcy%3Du8q8p7Wi2w%40mail.gmail.com.


--
Best regards,

Amol K.B
B.E(Mech), CSWIP 3.2.2, NACE CIP 1 & ASNT LII(4M)