GTAW + SMAW

67 views
Skip to first unread message

Jay Poojary

unread,
Jan 28, 2015, 4:28:14 AM1/28/15
to material...@googlegroups.com
Dear Experts,

Please clarify. If I have qualified a procedure with combination process i.e GTAW+SMAW for groove joint, then using this procedure can I allow to weld fillet joints using SMAW.



cordially,
Jay Poojary

Rudolf

unread,
Jan 28, 2015, 4:32:26 AM1/28/15
to material...@googlegroups.com
Using AWS  code NO. Using ASME  yes you have to write a new WPS  for single process.


Sent from Samsung Mobile
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAcO%3DyToxo3L--R8LjJ4aFCc2zrx8Yvo%2BE%2BMPFwzw%3DW8JLhZwQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

george....@gr.bureauveritas.com

unread,
Jan 28, 2015, 5:23:57 AM1/28/15
to material...@googlegroups.com

normally yes

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Saravanan Sornam

unread,
Jan 28, 2015, 10:01:31 PM1/28/15
to material...@googlegroups.com
Hi jay ,

Refer ASME Sec IX QW- 202.2 (C) , ofcourse you have to write a WPS Separately for SMAW for Fillet Welds, with the same PQR No.

Regards ,
Saravanan.



--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
Reply all
Reply to author
Forward
0 new messages