Dears,
Vessel joint efficiency is 0.85
Vessel RT requirement is Spot. 
Dished end having weld seam and fully RTd as the joint efficiency of head is 1 and other parts satisfied as per UW-52 spot RT requirements. So what would be the marking on name plate, RT3 or RT 4 or RT2.
Thanks in advance.
Manoj

PATEL JAVID

unread,
Jul 22, 2024, 7:55:58 AM7/22/24
to material...@googlegroups.com
RT4.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACgUO5k9Bu4LSKHgJCyfG-Mx33OCokwQRj3%2BpZZ09KwnRQSk7Q%40mail.gmail.com.

Saurabh Joshi

unread,
Jul 22, 2024, 8:33:33 AM7/22/24
to material...@googlegroups.com
Dear manoj 

       When some part of the vessel undergoes full RT and other part undergoes spot RT satisfying the requirements of UW-11 Asme sec VIII div.1 & where none of the other markings RT1, RT2 & RT3 is applicable then as per UG-116 vessel shall be marked as  "RT4".



Regards
S.Joshi

Mohd Siraj

unread,
Sep 6, 2024, 1:58:46 AM9/6/24
to Materials & Welding
RT-4.