API 650 radiography requirements

90 views
Skip to first unread message

TAMILSELVAN

unread,
Dec 3, 2024, 8:04:18 AM12/3/24
to Materials & Welding
API 650 standard for spot/full radiography- could anyone please  help to advise the RT % 

Hai Tran Ngoc

unread,
Dec 13, 2024, 9:42:24 AM12/13/24
to material...@googlegroups.com
Section 8, Para 8.1.2.3 for Horizontal butt joint, & para 8.1.2.9 for Bottom annular butt joint.
image.png


 

Thanks & Best Regards,


Hai, Tran Ngoc (Mr.)

E-mail: ngoch...@gmail.com
Telephone: +84-(0)977-881-880



Vào Th 3, 3 thg 12, 2024 vào lúc 20:04 TAMILSELVAN <tamilsel...@gmail.com> đã viết:
API 650 standard for spot/full radiography- could anyone please  help to advise the RT % 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/c95d1b29-a8f1-438b-9943-22d61704b4abn%40googlegroups.com.

Hai Tran Ngoc

unread,
Dec 13, 2024, 9:42:35 AM12/13/24
to material...@googlegroups.com
RT ratio according to API-650, it's very clear at section 8, para 8.1.2.2.
image.png


 

Thanks & Best Regards,


Hai, Tran Ngoc (Mr.)

E-mail: ngoch...@gmail.com
Telephone: +84-(0)977-881-880


Vào Th 3, 3 thg 12, 2024 vào lúc 20:04 TAMILSELVAN <tamilsel...@gmail.com> đã viết:
API 650 standard for spot/full radiography- could anyone please  help to advise the RT % 

--