channels and bonnets with six or more tube passes

58 views
Skip to first unread message

manohar matcha

unread,
Apr 5, 2022, 5:52:44 AM4/5/22
to materialswelding
Dear Group Members,

Please share your opinion/interpretation on API 660 Clause 9.6.9 (a)


 
Tube passes to be considered for individual channel or both channels (if Exchanger is having 2 channels)?
 
in other words:
Individual Channel passes to be considered or cumulative passes for both channels to be considered..?

Regards,
Manohar.

 

Raghuram Bathula

unread,
Apr 5, 2022, 6:07:46 AM4/5/22
to Materials-Welding
it is from one end of HE to another end is consider as 1 pass (not individual channel)

--

manohar matcha

unread,
Apr 5, 2022, 7:06:45 AM4/5/22
to material...@googlegroups.com
Please look into the attachment and advise that pwht is applicable for these channels as per API 660 clause 9.6.9 (a) or not?
Both channels are belongs to one HE.
Regards,
Manohar.

ClauseFrom: Raghuram Bathula <raghura...@gmail.com>
Sent: Tue, 05 Apr 2022 15:37:49
To: Materials-Welding <material...@googlegroups.com>
Subject: Re: [MW:33030] channels and bonnets with six or more tube passes
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubkQWFGHa70Wg-rztp22TzE0fmybM=5PWPP0yj...@mail.gmail.com.
CCE_000542.pdf

Raghuram Bathula

unread,
Apr 5, 2022, 7:13:54 AM4/5/22
to Materials-Welding
since it is 6 pass, required

Materials & Welding

unread,
May 4, 2022, 12:24:41 AM5/4/22
to Materials & Welding
Screenshot 2022-05-04 095405.jpg