WELD VISUAL INSPECTION-ACCEPTANCE CRITERIA---ASME VIII
1,264 views
Skip to first unread message
rahoof hassan
unread,
Nov 13, 2012, 7:33:09 AM
11/13/12
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to material...@googlegroups.com
Dear All,
Can someone give the Reference Standard or clause for Weld Visual Acceptance Criteria as per ASME VIII
--
with regards,
Rahoof Hassan,
Abu Dhabi, UAE
Theanh Lai
unread,
Jul 2, 2015, 8:01:54 AM
7/2/15
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to material...@googlegroups.com
Please see ASME VIII-UW-35 carefully. you will see thing which you need