https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/f0bb15a1-0ff5-4d62-b662-1b365472aadbn%40googlegroups.com.
Thanks & Regards
J.Gerald Jayakumar
0091-8838619635
Thanks & Regards
J.Gerald Jayakumar
0091-8838619635
AWS D1.1 does not restrict the number of PQRs supporting a WPS. Clause 6 requires only that essential variables be validated by procedure
qualification testing. Where a single PQR does not cover all required variables of a production WPS, multiple PQRs may be combined to provide
full technical support. Therefore, using multiple PQRs to support one WPS is fully acceptable and code-compliant.
Sridhar.