RT of Branch connection,

Skip to first unread message

nilesh

unread,
Mar 8, 2011, 5:00:17 AM3/8/11
to material...@googlegroups.com
Dear All,
 
            One of our client is asking Radiographic testing for branch connection full penetration weld.Kindly share your experience if anybody has done RT for this type of joint.Kindly describe the method how to do it if it is possible.
 
thanks and regds

  Nilesh Parsekar,
 

Fitria Rahman

unread,
Mar 8, 2011, 5:50:33 AM3/8/11
to material...@googlegroups.com
Hi Nilesh

Is your branch connection forms a 90 degree angle? Am I right?
as far i know, you can not carrying out RT. The films shall be placed on flat surface (or near flat) or longitudinal joint.


2011/3/8 nilesh <nilesh_...@yahoo.com>

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

samshuddin k

unread,
Mar 8, 2011, 7:14:31 AM3/8/11
to material...@googlegroups.com, nilesh
Dear sir
It is possible to take RT for branch connection,by DWSI (double wall single image technique) 


Samshiddin.K
Bharati shipyard Ltd
Mangalore

ARIVALAGAN ARIVALAGAN

unread,
Mar 9, 2011, 12:02:35 AM3/9/11
to material...@googlegroups.com
Hi,
  why not it is possible. but the film review to be differences. it will not give  
100% correct condition.little bit similar. the film review person to be understand.

V.Arivalagan.
Welding Inspector,
SK E&C,
Kuwait.

Fitria Rahman

unread,
Mar 9, 2011, 8:29:05 PM3/9/11
to material...@googlegroups.com
hi Nilesh
After i read "branch connection", my assumption was a "T" joint, like a joint in TKY in structural welding. As i wrote in first reply, you can not carrying out RT.
If you're talking about butt weld, OF COURSE, you can carrying out RT.

Rgds,