Charpy Test of Inconnel (ASME B 31.3)

171 views
Skip to first unread message

Ilkin Hasanov

unread,
Mar 31, 2021, 6:25:51 AM3/31/21
to material...@googlegroups.com
Hi All,
Could you please advise, when does ASME B31.3 require to perform Charpy Test for Inconel Material (UNS 06625)? 

After which MDT it is mandatory to perform it? 


Regard, 
Ilkin HASANOV.

Customer Care

unread,
Apr 1, 2021, 2:51:58 AM4/1/21
to material...@googlegroups.com

Dear Ilkin,

 

The alloy 625 (Ni-Cr-Mo-Nb) for high temperature service 0-800 C and highly corrosive environment, rarely requires impact testing. ASTM B564 (UNS NO6625) does not state it as proof of its mechanical properties. If this is your case, at what temperature would you perform the Charpy test?

Better: in what temperature range is the service of this alloy located, in your case?

 

Regards,

Ramon Briceno.

 

 

 

Sent from Mail for Windows 10

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADrxeDYXdxMbYXHYBV%2BRaKidjv7B%2BB_x7%3Dw8Mz5h1k-Nm%2BfiQg%40mail.gmail.com.

 

Reply all
Reply to author
Forward
0 new messages