Looking for Expert OPINION for the Crack

38 views
Skip to first unread message

Chaudhary Zafar Iqbal

unread,
Apr 18, 2023, 11:04:46 PM4/18/23
to material...@googlegroups.com
Dear Welding Expert ,

Greetings of the Day,

Looking for the expert opinion for the CRACK.
Material: ASTM A210 GR-1



image.png

image.png



Best Regards,

M.Zafar Iqbal

00966544639978

james gerald

unread,
Apr 19, 2023, 4:41:53 AM4/19/23
to material...@googlegroups.com
These are simple boiler carbon steel. Looks like centerline crack, results from excessive weaving, what is your bead width to depth ratio.

Thanks & Regards

J.Gerald Jayakumar



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP9k9Xf%2BbFhAurChV6NMgTBs9vyo6%3DUhBqDHZMb-DQMJ-9vzvA%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages