Minimum leak path test

1,513 views
Skip to first unread message

krishna mudhale

unread,
Sep 10, 2012, 10:07:55 AM9/10/12
to material...@googlegroups.com
Dear experts, How to calculate minimum leak path (MLP) for tube to
tube sheet joint,please give me refrence also . Thanks &
regards- krishna mudhale.

Chandrashekhar Kumar

unread,
Sep 10, 2012, 12:02:23 PM9/10/12
to material...@googlegroups.com
MLP is 1.4*tube thickness
> --
> To post to this group, send email to material...@googlegroups.com
> To unsubscribe from this group, send email to
> materials-weld...@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
>

sevak hiren

unread,
Sep 11, 2012, 2:08:28 AM9/11/12
to material...@googlegroups.com
Dear,

Leak path dimension is not mentioned in ASME section IX.

As per ASME Section IX, QW-193.1.3 Acceptance Criteria — Macro- Examination.

Using a minimum of 10X magnification, the exposed cross sections of the weld shall confirm

(a) minimum leak path dimension required by the design

Please refer EEMUA standard for better understanding & requirements for Tube to Tube sheet welding procedure.

EEMUA standard, clause no.3.2.1 - Visual Examination

On polishing & etching the section, the minimum throat thickness or leak path of each weld shall not be less than 0.7t, where t is the nominal wall thickness of the tube.

Regards

Hiren Sevak




Durgesh Gaonkar

unread,
Jan 20, 2015, 7:30:27 AM1/20/15
to material...@googlegroups.com, durge...@gmail.com
Dear All, 

how to calculate minimum leak path for tube to tube sheet mockup test
Tube Thk : 1.65 mm
Tube-sheet : 50 mm

please provide formula

Durgesh Gaonkar
Reply all