GTAW weld weaving

1,269 views
Skip to first unread message

simon lawrence

unread,
Mar 31, 2016, 7:30:12 AM3/31/16
to Materials & Welding
Pls confirm that Weld weaving width ,  weld weave maximum how much we can accepted in GTAW process ?

Jim Price

unread,
Mar 31, 2016, 8:19:52 AM3/31/16
to material...@googlegroups.com

You won’t find a specific para for weave width, other than ASME section 9, relating to your WPS that has been qualified.  Maximum weave width shall be as stated in your WPS (welding procedure). 

I believe this will be true for other Standards.

 

Best Regards,

 

 

Jim Price | Welding Engineer, CWI

Direct:  320.7463439 | Fax: 417-862-5564

jimp...@polarcorp.com

cid:image001.jpg@01D0E005.E9837830

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/757ab274-8b90-4e73-93a9-35e7c078e57f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

pkkani...@gmail.com

unread,
Apr 1, 2016, 12:45:35 AM4/1/16
to Materials & Welding
As per sec IX 2.5 times of the electrode dia can be allowed for weaving . In case of GTAW you can consider the tungsten dia in place of electrode dia.

Kannayeram Gnanapandithan

unread,
Apr 1, 2016, 12:45:55 AM4/1/16
to material...@googlegroups.com

Generally 10mm

On 31-Mar-2016 5:00 pm, "simon lawrence" <simonla...@gmail.com> wrote:
Pls confirm that Weld weaving width ,  weld weave maximum how much we can accepted in GTAW process ?

--

jaya anil

unread,
Apr 1, 2016, 12:46:48 AM4/1/16
to material...@googlegroups.com
As per Section IX, Weld Weaving is non essential variable for GTAW process. 

As such it is based on your WPS  which was qualified and recorded . If your job is having , Notch Toughness requirement, then dont go for more weaving which will reduce toughness properties. Go with multi layers .

Thanks

On Thu, Mar 31, 2016 at 3:29 PM, simon lawrence <simonla...@gmail.com> wrote:
Pls confirm that Weld weaving width ,  weld weave maximum how much we can accepted in GTAW process ?

--

Sathish Jaganathan

unread,
Apr 1, 2016, 2:02:45 AM4/1/16
to material...@googlegroups.com
Hi

Please refer ASME SEC II- C page no 133 & 138 (*Notes)


For more options, visit https://groups.google.com/d/optout.



--
Thanks & Regards.....,
J.Sathish
QC Inspector ( Mechanical)
Gulf Petrochemical Services & Trading LLC.
Mob no:-+968-96371006

Alternate Email:- sathishj...@yahoo.com
Oman


Kannayeram Gnanapandithan

unread,
Apr 1, 2016, 2:02:54 AM4/1/16
to materials-welding
generally for GTAW-- 1.5 X Nozzle ID

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Fri, Apr 1, 2016 at 10:55 AM, Kannayeram Gnanapandithan <kgpan...@gmail.com> wrote:
Sec IX, has nowhere said about weaving width for any welding process, but in Section 1 and Section 8, it has given for welding by SMAW, the weaving width may be 4Xcore dia.  

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.

Kannayeram Gnanapandithan

unread,
Apr 1, 2016, 2:14:49 AM4/1/16
to materials-welding
which edition??

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

JIJILAL K M

unread,
Apr 2, 2016, 3:24:53 AM4/2/16
to material...@googlegroups.com
In general practice ,the weaving width is limited to 2.5 to 3 times the dia. of filler wire used in GTAW 

JIJILAL K.M. 
QA/QC Manager,
Thai Jurong Engineering Ltd,
KCE SPP Project,Thailand



On 31 March 2016 at 16:59, simon lawrence <simonla...@gmail.com> wrote:
Pls confirm that Weld weaving width ,  weld weave maximum how much we can accepted in GTAW process ?

--

Kannayeram Gnanapandithan

unread,
Apr 2, 2016, 3:48:19 AM4/2/16
to materials-welding
no KMJ, nowhere it is given like what u have said

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

Jim Price

unread,
Apr 4, 2016, 10:44:31 PM4/4/16
to material...@googlegroups.com

Nowhere found this is why you need to specify weave or stringer.

Weave width needs to be included.

 

Best Regards

 

Jim Price | Welding Engineer, CWI

Direct:  320.7463439 | Fax: 417-862-5564

jimp...@polarcorp.com

cid:image001.jpg@01D0E005.E9837830

 

 

 

 

 

Ramesh Barot

unread,
Apr 5, 2016, 2:43:45 AM4/5/16
to JimP...@polarcorp.com, material...@googlegroups.com

Dear All experts,

Kindly conclude....the matter because many of us have same query for GTAW.


Thanks

Ramesh Barot


Sent from my LG Mobile


------ Original message------

From: Jim Price

Date: Tue, 5 Apr 2016 08:14

To: material...@googlegroups.com;

Subject:RE: [MW:24630] GTAW weld weaving


Nowhere found this is why you need to specify weave or stringer.

Weave width needs to be included.

 

Best Regards

 

Jim Price|Welding Engineer, CWI

Direct:  320.7463439| Fax: 417-862-5564

jimp...@polarcorp.com

file:///data/data/com.lge.email/data/Messaging/Data/Email/1223208520/

Vishwas Keskar Welding Manager Pune India

unread,
Apr 17, 2016, 11:07:55 AM4/17/16
to Materials & Welding
ASME SEC IX is lenient on weaving.WPS will guide this . Put the maximum weaving width  in WPS . With 2.4 dia , filler wire , a width of @12 mm is an acceptable width    


On Thursday, March 31, 2016 at 5:00:12 PM UTC+5:30, simon lawrence wrote:

Kannayeram Gnanapandithan

unread,
Apr 18, 2016, 1:24:32 AM4/18/16
to materials-welding

On what basis it is acceptable, any ref pl

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.

chandan sharma

unread,
Apr 18, 2016, 1:24:32 AM4/18/16
to material...@googlegroups.com

Its depends on the PQR.
Weaving tends to increase the heat input on the material.

--

Prakash Hegde

unread,
Apr 18, 2016, 1:26:29 AM4/18/16
to material...@googlegroups.com
Hi!
As such no code address about weaving but emphasis on heat in put
I) Excessive weaving increases heat input Good
ii) Good welding practices suggest about min weaving to reduce heat input viz about 2-3 time the electrode dia
Still  in spite of more weaving, if you can achieve good impact value No problem  and no body should object However experience says it is difficult to achieve consistence Impact result with excessive weaving
Regards
Hegde



--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.

Vishwas Keskar Welding Manager Pune India

unread,
Apr 24, 2016, 11:50:48 PM4/24/16
to Materials & Welding
Normal weaving by manual GTAW is @12 mm, which shall be addressed in WPS

Vishwas Keskar


On Thursday, March 31, 2016 at 5:00:12 PM UTC+5:30, simon lawrence wrote:

khalidzu...@gmail.com

unread,
Dec 22, 2019, 2:24:12 AM12/22/19
to Materials & Welding
Please refer PQR information. Width is advisable as per pqr record.

On Thursday, March 31, 2016 at 3:30:12 PM UTC+4, simon lawrence wrote:
Reply all
Reply to author
Forward
0 new messages