Essential variables for Welding Procedure as per API 1104 22nd edition

1,192 views
Skip to first unread message

Babur Khan

unread,
Sep 27, 2021, 7:43:39 AM9/27/21
to material...@googlegroups.com
Greetings,
As per Latest’s edition of API 1104 (22nd edition) Table 1 Essential variables for qualification of welding procedure Specifications, Diameters are not listed as a essential variables.
Please share your experiences with standard references for diameter of Pipe are essential variables or not as per API 1104?
image0.jpeg

Mohd Siraj

unread,
Feb 13, 2022, 10:17:43 PM2/13/22
to Materials & Welding
it's essential for welders only.
for WPS, diameter is not essential.