Greetings,

 

 Code: ASME IX

Process: GTAW

Diameter: DN50

Specs: ASTM A106

Qualification Status: expired

 

As per QW 322.2

    Providing the conditions of QW-304 and QW 305 are satisfied, renewal of welder qualification under QW-322.1(a) may be done on production work.

 

QW 304

     Alternatively, welders making a groove weld using SMAW, SAW, GTAW, PAW, and GMAW (except for short circuit mode) or combination of these process maybe qualified by radiograph examination,

 

 Does this sentence applied if the welder has welded the following 3 months prior to his expiration of his ASME qualification, welding as per below:

Code: DNV-OS-F101

Process: GTAW

Diameter: DN50

Grade: DNV 450

 

 

Can the welder  renew his qualification on production work as per QW 322.2, under this circumstances?

 

Does this production work means that it is the work that needs qualified welders to do the work?

 

 

 

 

Thank you in advance.

 

 

 

 

Cheers,

 

Larry

ALAP M

unread,
Nov 10, 2010, 3:21:12 AM11/10/10
to Materials & Welding
YES .

The welder can be qualified on the basis of work done by him within
the period of 6 months( before expiration of his certificate).

Interpretation of QW 322 -"if the welder has not welded more than 6
months - or absent from work, his certification expires and has to be
Re-Qualified, can not be Renewed"


Regards,

Alap Mistry

muthu barathi

unread,
Nov 10, 2010, 4:47:16 AM11/10/10
to material...@googlegroups.com

hi,

first say whether the said welder is performing welding? if so take a RT ON THE JOB and qualify code permits. if the welder performs welding continuosly without any repair qualification may be performed based on his RT or UT as per job requirement. you can revalidate the certificate.



On Wed, 10 Nov 2010 12:12:25 +0530 wrote
--
>
To post to this group, send email to material...@googlegroups.com
>
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>


Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951
Reply all
Reply to author
Forward
0 new messages