Dear all,

what will happen to the grains of a ferritic stainless-steel type AISI 405 used as an attachment of a hanger bar in a boiler, when it is exposed to flame temperatures of the boiler for 4 years of continuous operation? It is understood that the 405 steel will not oxidize in the high-temperature service environment.

Regards,

Emad


Ahmed Osman

ungelesen,
25.01.2021, 00:46:1325.01.21
an material...@googlegroups.com
may get :-
 *  grain growth which lead to low toughness 
 *  brittle phases as Sigma or Chi which lead to loos of toughness or even cracking 

Best Regards ,
ENG. Ahmed Osman


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABtwbJG4D61j93y-Onv4L1kOjgxaAhSTDaCUgJ_9MjhzSm_4nA%40mail.gmail.com.

Vishwas Keskar

ungelesen,
26.01.2021, 01:45:1226.01.21
an material...@googlegroups.com
Is welding involved ?
If yes , what welding procedure ?
Pl. let us know 

What thickness are involved ?

Vishwas Keskar Welding Manager WELDING

ungelesen,
31.01.2021, 22:13:5231.01.21
an Materials & Welding
These are straight Cr Stainless steels for high temperature application.
In boiler , you can use this material.
Pl. send what attachment part you are looking for ?

EmaD FaRaHanI

ungelesen,
31.01.2021, 22:31:1331.01.21
an material...@googlegroups.com
Thank you for your answer. I was wondering what would happen to grains of stainless steel 405 grains as hanger in boiler  when they exposed to high temperature for long time?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

pgos...@rogers.com

ungelesen,
31.01.2021, 22:54:2031.01.21
an material...@googlegroups.com

Hi Emad,

 

Your query does not provide details about design/working condition.405 is a ferritic stainless steel. These steels have “good oxidation resistance “however lacks the ductility which is  well evident in austenitic stainless steel. 475 Deg embrittlement may be a possibility upon prolonged exposure @ 500 Deg or more. Read the attached extract from API-RP-571 and proceed for any inspection/ damage assessment as required.

 

Hope this would be of help.

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent  & Consulting Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgos...@rogers.com,pradip....@gmail.com

Cell/Whasapp:1-905-9793232

Section_4 General Damage Mechanisms_475Deg C Embrittlement.pdf
Allen antworten
Antwort an Autor
Weiterleiten
0 neue Nachrichten