Impact Test Requirement : ASME Sec. VIII Div.1

86 views
Skip to first unread message

williams p wilson

unread,
Sep 29, 2022, 11:38:22 PM9/29/22
to material...@googlegroups.com
Dear Experts, 

Please share the Impact Test requirements of SA 516 Gr.70 N , 80 mm thickness with a MDMT of -29 degree C.

Thank You & Regards
Williams P Wilson
QA/QC Engineer
Please consider the environment before printing this message

Pravin Kurade

unread,
Sep 29, 2022, 11:55:25 PM9/29/22
to material...@googlegroups.com
Yes impact is required ref UG 84 chart

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ7-ZGwD2T5SHytyTQndeSpueg2kxmG%3DJg5S6cKHMspPUg%40mail.gmail.com.
--
Pravinkumar kurade

williams p wilson

unread,
Oct 3, 2022, 12:22:53 AM10/3/22
to material...@googlegroups.com
Dear Sir,


Wt will be the test temperature and the acceptance criteria to procure the material.

srinivas rao

unread,
Oct 6, 2022, 5:13:56 AM10/6/22
to material...@googlegroups.com

Dear Williams ,

Test temperature generally it will be mentioned in client specification for impacting of procedures if client wants at different temperature based on their service requirements 

or else Test temperature will be the same as MDMT of base material 

for test specimen extraction refer UG-84 fig , number of specimens will vary based on welding procedures used during welding and thickness of deposition, way of welding - single side/double side


Thanks & Regard, 
Srinivas Rao
Welding Engineer 

williams p wilson

unread,
Oct 6, 2022, 6:02:56 AM10/6/22
to material...@googlegroups.com
Dear Sir,

Thanks for your mail.

Our case the 80 mm thick, normalized carbon steel plate will undergo RN, SR1 & SR2
So, do we need to consider higher impact values during the selection of plates.

Thank You & Regards
Williams P Wilson
QA/QC Engineer
Please consider the environment before printing this message

srinivas rao

unread,
Oct 6, 2022, 7:02:06 AM10/6/22
to material...@googlegroups.com
Dear Williams, 
each heatrement  type RN & SR qualification procedures you need to do all the testing .. 
check client specification are they asked to carry out complete test at SR1 & SR2 , if not u can carry out all the testing for SR2 and only impact , Macro & hardness Tests at SR1 (agree same with client) 

in general these plates will be guaranteed and test at - 51deg C in normalised condition , specify this requirement during purchase of BM & welding consumables
at the time of procurement u need to specify your project heat treatment conditions clearly to vender /supplier that material shall guarantee 2 cycle PWHT and 

Regards,
srinivas Rao
welding Engineer 