RT joint with painting

175 views
Skip to first unread message

sanks...@gmail.com

unread,
Oct 20, 2022, 11:13:28 PM10/20/22
to Materials & Welding
Gents,
    i have query , We can do RT for weld Joint with painting , Its allowed , In our site they did RT with painted joint with out client approval 
    They will be problem that may hide weld defect , painting DFT 300 to 400 micron
If allowed do RT with Painting , Please share some supporting documents 

Thanks for your support 
Best regards
Sankar.k

Babur Khan

unread,
Oct 21, 2022, 1:55:40 AM10/21/22
to material...@googlegroups.com
Greetings,
Yes you can do RT with Paint.
Coating or painting can hide only visual defects. 
Buried defects can be detected with RT.  

Muhammad Babur Khan

Sent from my iPhone

On 21 Oct 2022, at 6:13 AM, sanks...@gmail.com <sanks...@gmail.com> wrote:

Gents,
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ac980cb1-6c30-40ef-8a12-5c5cbcc44700n%40googlegroups.com.

Perumal Govindan

unread,
Oct 21, 2022, 4:12:33 AM10/21/22
to material...@googlegroups.com
Hi
Your Client only can decide this issue, speak with them and resolve otherwise retake after paint removal.

Regards 
Govindan Perumal 

sanks...@gmail.com

unread,
Oct 30, 2022, 11:12:20 PM10/30/22
to Materials & Welding
How we can prove it , There is any documents that's says about with painting can perform RT for Weld Joint, When we propose to client we have to submit some supporting documents 
If you have any supporting documents , Please share with me 

kingslygeo vargheese

unread,
Feb 3, 2023, 1:40:40 AM2/3/23
to material...@googlegroups.com
ITP / Procedure sequence was not followed.
Considering the repair after the painting will double the job ( 3 times blasting - Initial / paint removal before repair/blasting for painting).
So the Construction manager and company can decide.

ITP / Procedure has to be revised and approved ( Normally the client will not approve )

Regards,
V. Kingsly Geo.