The detection of defects by RT is limited by a certain number of factors like:
Density
Penetration
Geometrical unsharpness
You have to thoroughly review your RTs for Code compliance
best regards
Dr. Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE
Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
"'raouf salhi' via Materials & Welding" ---03/02/2015 05:10:16---Dear experts; We have a skid of piping 10 " and 2 " API 5L welded and inspected according B 31.3.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/581386843.973075.1422885025165.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.
This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com
Agree with Georgios.
As complement you could inspect your welded joint with advance ultrasonic testing (phased-array). This is a volumetric inspection method too, and with correct transductor and personnel, you could have a good precision to evaluated and categorize the indication using acceptable and non-acceptable criteria from B31.3
regards
Miroslav Tadic
Integrity Enginner
CEE
Gerencia de Producción - Mantenimiento
YPFB Chaco S.A.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/OF67436E33.0532C53D-ONC2257DE1.002CA9BF-C2257DE1.002CDBBE%40LocalDomain.