Pickling and passivation

104 views
Skip to first unread message

Nikesh ransinh

unread,
Nov 4, 2010, 4:07:48 AM11/4/10
to Materials & Welding
hello !
for pickling and passivation for 304L matial which chemical to be
used ? and what is the ratio whith water of the chemical ?

cyril andrews

unread,
Nov 5, 2010, 2:19:34 AM11/5/10
to material...@googlegroups.com
Hi,
According to my knowledge I answered and attached some details to your
query. The pickling gel details are below and the percentage of water shall
be 1 part of gel with 3 parts of water or 1 parts of water. But i will be
provided in MSDS. Please check to it and proceed.

PICKLING GEL
The pickling gel is of two types,
1. Avesta Spray pickling gel 204.
2. Avesta Pickling gel 122.
3. Avesta BlueOneR Pickling Paste 130
4. Avesta Pickling Paste 101
5. Avesta BlueOneR Spray Pickle Gel 230
6. Avesta GreenOne Spray Pickle Gel 220
7. Avesta Spray Pickle Gel 215
8. Avesta Spray Pickle Gel 204
9. Avesta Spray Pickle Pump SP-25
10. Avesta Indicator 701

Spray Pickling Gel
Pickling Gel 204 (HNO3 15-25% & HF 1-8%) shall be used in general
areas. The pickling Gel applied on dry surface.

PASSIVATION AGENT
Passivation AGENT 601(HNO3 20-50%) shall be used. Trained and
skilled personnel will carry out the exercise.


Regards,

J.C.Andrews,
QA/QC Engineer,
Doha-Qatar.

hello !
for pickling and passivation for 304L matial which chemical to be
used ? and what is the ratio whith water of the chemical ?

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to
materials-weld...@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

Pickling.doc
PICKLING GEL 122-SPECS.pdf

M.Shankar

unread,
Nov 5, 2010, 2:31:21 AM11/5/10
to material...@googlegroups.com
Hi
Hope that below links will help you.


Regards/Shankar



From: Nikesh ransinh <niker...@gmail.com>
To: Materials & Welding <material...@googlegroups.com>
Sent: Thu, 4 November, 2010 4:07:48 PM
Subject: [MW:8068] Pickling and passivation

hello !
for pickling and passivation for 304L matial which chemical to be
used ? and what is the ratio whith water of the chemical ?

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsub...@googlegroups.com

Bisso, Giuseppe

unread,
Nov 5, 2010, 4:27:04 AM11/5/10
to material...@googlegroups.com

Please check ASMT A 380.

Now used also solutions with hydrogen peroxide (high volumes/concentrations).

 

Joseph B.

Materials & Welding Eng.

 


Da: material...@googlegroups.com [mailto:material...@googlegroups.com] Per conto di M.Shankar
Inviato: venerdì 5 novembre 2010 7.31
A: material...@googlegroups.com
Oggetto: Re: [MW:8082] Pickling and passivation

To unsubscribe from this group, send email to materials-weld...@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



This e-mail contains privileged and confidential information intended for the use of the addressees named above. If you are not the intended recipient of this e-mail, you are hereby notified that you must not disseminate, copy or take any action in respect of any information contained in it. If you have received this e-mail in error, please notify the sender immediately by e-mail and immediately destroy this e-mail and its attachments.

RMK

unread,
Nov 8, 2010, 1:53:30 AM11/8/10
to material...@googlegroups.com
Hi,
Find the attached book will be useful to select the right product as per the grade specification .If you need further you can contact Bohler Welding Group Middle East Office or BWG Local Distributor .

Thanks & Regards ,
Muthu,
Bohler -Dubai .
Mb: +971 50 100 63 50
If you need further details visit www.bwgme.com
Avesta Pickling Handbook .pdf
Reply all
Reply to author
Forward
0 new messages