Thickness Range for WPS

222 views
Skip to first unread message

Mohd Azam

unread,
Jan 22, 2015, 6:24:19 AM1/22/15
to material...@googlegroups.com

Dear Experts,

The PQR is qualified on as per ASME SEC IX and ASME B31.3 requirement & . Thickness criteria is to followed as per ASME B31.3:

 

P. No. 1 GR.1 (A106 Gr.B) to  P. No. 1 Gr.2 (A105N),

Impact @ -20 Deg C as per project specification requirement

 

Thickness for WPS 1.5 mm to 20 (T to 2T) mm or 5 to 16 mm (T/2 to T+6).

 

Kindly give the code reference:

 

 

Thanks & Regards,

Mohd. Azam

george....@gr.bureauveritas.com

unread,
Jan 22, 2015, 7:18:28 AM1/22/15
to material...@googlegroups.com

Τ/2 to T + 6 (see table 323.3.1)
you will never find impact test qualification requirements and ranges  in Section IX. Always in the construction Code Section

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Inactive hide details for Mohd Azam ---22/01/2015 13:30:46---Dear Experts, The PQR is qualified on as per ASME SEC IX and ASME Mohd Azam ---22/01/2015 13:30:46---Dear Experts, The PQR is qualified on as per ASME SEC IX and ASME B31.3 requirement & .

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CABD%2BRXS46ip-dH%3Dg2d0P_AyhtA4PaWkVNavRCUT0YH%3DAWoGs0g%40mail.gmail.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Mohd Azam

unread,
Jan 22, 2015, 10:30:30 AM1/22/15
to material...@googlegroups.com
Pls refer QW403.6 for SMAW process, Impact testing. MY question is for CS material only not LTCS

Thickness range 1.5 mm to 2T or T/6 to 2T

Thanks & Regards,
Mohd. Azam