Filler wire for welding off SA182F11 to SA268TP446

78 views
Skip to first unread message

sujit kumar

unread,
Feb 13, 2025, 8:11:12 AM2/13/25
to material...@googlegroups.com
Hello experts

Greetings for the day.


Kindly please tell me what will be the filler wire for welding of
SA182F11 to SSA268 TP446




Best regards
Sujit kumar

sridhar cn

unread,
Feb 13, 2025, 9:51:44 PM2/13/25
to material...@googlegroups.com
ERNiCr-3 (Inconel 82)  for corrosion resistance or  ERNiCrMo-3 (Inconel 625)  for corrosion resistance 
and extreme environments, or ER309L  for general purpose could be used.
Preheating  & interpass temp. control will help  to minimize the risk of cracking.  PWHT might be necessary 
to relieve stresses and improve the weld properties.
Sridhar.
-------------------------------------------------------------------------------------------------------------------------------------


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAFonYWPKQrt%2Ba3WvcLqQNQA%2BWW6KBw649UUC_Nh2xdcpwHPhzw%40mail.gmail.com.

sujit kumar

unread,
Feb 20, 2025, 2:23:17 AM2/20/25
to material...@googlegroups.com
Hello Sridhar,

Thank you so much for your response.
May I know the source how you have selected that filler wire for SA182F11 to SA268TP446 welding....if you have any document regarding that could you please share that document. I will be grateful to you.



Thanks and regards
Sujit kumar

sridhar cn

unread,
Feb 20, 2025, 6:45:54 AM2/20/25
to material...@googlegroups.com
Dear Mr. Sujit Kumar,
The details are sourced from Welding handbooks.
I am enclosing a part of it for your records.
rgds,
C S
---------------------------------------------------------------------

WELDING CS TO SS FILLER WRES -THREAD.docx