WPQR as per EN 15614-1

314 views
Skip to first unread message

Vijay Katkar

unread,
Sep 15, 2015, 6:42:56 AM9/15/15
to material...@googlegroups.com
Dear All,

Need your assistance,

I have qualified WPQR for fillet weld (Plate to Plate) as per EN 15614-1.

Can i use this PQR to weld pipe (15 mm OD) to plate for fillet weld (thickness range is within specified limit)?

Please guide me on this.

Thank you

Vijay Katkar 

Jay Poojary

unread,
Sep 15, 2015, 7:50:53 AM9/15/15
to material...@googlegroups.com
Dear All,

It seems ok. Can be done. Please correct me, if I am wrong.





cordially,
Jay Poojary

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP37wrJHuASs4hgSdXXR17aezNU0bkbmBZcVfgC8nuBCMzPWfQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Eknath Kharat

unread,
Sep 15, 2015, 8:01:33 AM9/15/15
to material...@googlegroups.com

Definitely You can do but consider thickness range
Eknath

--

george....@gr.bureauveritas.com

unread,
Sep 15, 2015, 9:05:41 AM9/15/15
to material...@googlegroups.com

In EN 15614-1 the diameter is a qualification parameter (contrary to ASME IX).
Please check 8.3.2.3 of EN 15614-1

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Inactive hide details for Vijay Katkar ---15/09/2015 13:43:02---Dear All, Need your assistance,Vijay Katkar ---15/09/2015 13:43:02---Dear All, Need your assistance,

--

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to


To post to this group, send email to


To view this discussion on the web visit

https://groups.google.com/d/msgid/materials-welding/CAP37wrJHuASs4hgSdXXR17aezNU0bkbmBZcVfgC8nuBCMzPWfQ%40mail.gmail.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

hpi001

unread,
Sep 15, 2015, 12:48:56 PM9/15/15
to Materials & Welding
If you have to weld a fillet weld arround pipe or bar material than you need to have a qualification in which also the diameter is qualified as well.

Vijay Katkar

unread,
Sep 15, 2015, 11:16:13 PM9/15/15
to material...@googlegroups.com

Thank you for your valuable reply.

But I didn't understand why do we need separate Qualification for Pipe fillet joint.

What will be the consideration behind this?

Need your guidance.

Best regards

Vijay Katkar

Kannayeram Gnanapandithan

unread,
Sep 16, 2015, 5:09:01 AM9/16/15
to materials-welding
Jay. could u pl mention para in the STD

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

Kannayeram Gnanapandithan

unread,
Sep 16, 2015, 5:13:26 AM9/16/15
to materials-welding
that is for butt joints???, is it same for fillet also

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

george....@gr.bureauveritas.com

unread,
Sep 16, 2015, 6:10:43 AM9/16/15
to material...@googlegroups.com

because of the diameter.
If your diameter would be larger than 500 mm or when the diameter is > 150 mm and the position are PA or PC position then you would not need a new qualification



best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04

Vijay Katkar

unread,
Sep 16, 2015, 6:53:21 AM9/16/15
to material...@googlegroups.com
ok sir,

Now we have fillet welding of 6mm dia rod with plate .

Do we need do qualification of Rod diameter as per  EN 15614-1?

Thank you

Vijay Katkar
 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.

Kannayeram Gnanapandithan

unread,
Sep 16, 2015, 7:37:27 AM9/16/15
to materials-welding
is it for fillet also Mr George

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Wed, Sep 16, 2015 at 3:18 PM, <george....@gr.bureauveritas.com> wrote:

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
Reply all
Reply to author
Forward
0 new messages