do we need seperate wps for repair

755 views
Skip to first unread message

anil kumar

unread,
Oct 17, 2016, 12:20:10 AM10/17/16
to Materials & Welding
Hi,

       Do we need separate wps for repair or the wps we used in production will be sufficient as per ASME B31.3,
and using the  PQR which used in production , can I qualify repair wps.

Thank you
ANIL KUMAR

Nitin Patil

unread,
Oct 17, 2016, 12:35:37 AM10/17/16
to material...@googlegroups.com

U need not prepare separate wps for repair

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/083fabc6-d945-43b4-ab2b-a50ffd3cec46%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

venkat chikkala

unread,
Oct 17, 2016, 12:43:05 AM10/17/16
to material...@googlegroups.com
Dear,

We may use the same procedure for repairing the welds as per clause 328.6 ( If there is no special requirement from client), which say

328.6 Weld Repair
A weld defect to be repaired shall be removed to
sound metal. Repair welds shall be made using a welding
procedure qualified in accordance with para. 328.2.1,
recognizing that the cavity to be repaired may differ in
contour and dimensions from the original joint. Repair
welds shall be made by welders or welding operators
qualified in accordance with para. 328.2.1. Preheating
and heat treatment shall be as required for the original
welding. See also para. 341.3.3.

How ever this clause is applicable only for the systems which are not placed in service, Refer clause 300.

Intent of the Code

(1) It is the intent of this Code to set forth engineering
requirements deemed necessary for safe design
and construction of piping installations.
(2) This Code is not intended to apply to the operation,
examination, inspection, testing, maintenance, or
repair of piping that has been placed in service. The
provisions of this Code may optionally be applied for
those purposes, although other considerations may also
be necessary.


Regards,
CH V Ramana
BVIL


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.

prem_nautiyal26

unread,
Oct 17, 2016, 1:01:09 AM10/17/16
to material...@googlegroups.com
Hi

You only need to prepare the repair procedure wherein your production WPS will be referred.

Regards

Prem Nautiyal 





Sent from my Samsung Galaxy smartphone.

anil kumar

unread,
Oct 17, 2016, 1:01:09 AM10/17/16
to Materials & Welding
thank you sir for your reply
if possible can you explain these in the para 328.6"
recognizing that the cavity to be repaired may differ in
contour and dimensions from the original joint."


thank you

venkat chikkala

unread,
Oct 17, 2016, 8:29:43 AM10/17/16
to material...@googlegroups.com
Dear,

The statement in the clause 328.6 say, the grove shape of repair weld may be different from the original weld joint.

Regards,
CH V Ramana
BVIL




George Dilintas

unread,
Oct 18, 2016, 11:47:04 PM10/18/16
to Meghanadh K
Check paragraph 328.6 & 328.2.1.
Since grooves for repair could differ from grooves for production, you may need to write a new WPS. However, you may support this WPS with an existing PQR if the essential (and supplementary essential in case of impact requirements) variables match

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

Kannayeram Gnanapandithan

unread,
Oct 19, 2016, 4:20:42 AM10/19/16
to materials-welding
not required as per 328.6 and 328.2.1

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Tue, Oct 18, 2016 at 9:21 PM, George Dilintas <dili...@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (dili...@gmail.com) Add cleanup rule | More info

Check paragraph 328.6 & 328.2.1.
Since grooves for repair could differ from grooves for production, you may need to write a new WPS. However, you may support this WPS with an existing PQR if the essential (and supplementary essential in case of impact requirements) variables match
2016-10-17 7:05 GMT+03:00 anil kumar <anil...@gmail.com>:

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/083fabc6-d945-43b4-ab2b-a50ffd3cec46%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

Shashank Vagal

unread,
Oct 19, 2016, 4:20:42 AM10/19/16
to material...@googlegroups.com
Dear Sir,
These paragraphs refer to Sec IX in general with additional requirements from B31.3 and do not specifically state that a separate Repair WPS is required. However, most clients demand it. What we have done in such cases is to run 2 PQRs, one with test coupons (more than 1 usually) having repairs at various depths/sections as per the client requirements.
 
Best Regards,
Shashank C Vagal  (Quality Adviser)
Neo Metal-Analyst & NDT Services (Approved by IBR, Thermax, AERB)
Regd Office: 301, PRATHAMESH, M G Rd – Mahant Rd, Vile Parle East, Mumbai 400 057 INDIA
Tel: +91 22 2611 6640 / (+91) 9821386292 /  8082395502 / 9819191861    
Works Office: A-25, Geet Siddhee, Sector No. 11, Pradhikaran, Gat No. 62, Boradewasti, Moshi, Dist: Haveli, PCMC, Pune – 411044, Maharashtra, India   
www.neometalanalystndt.com / enq...@neometalanalystndt.com / nach...@yahoo.com




From: George Dilintas <dili...@gmail.com>
To: Meghanadh K <material...@googlegroups.com>
Sent: Tuesday, 18 October 2016 9:21 PM
Subject: Re: [MW:25561] do we need seperate wps for repair

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40BLudc1iHYek3JRXv_BwvK7hxRyTp3i5FnUr5AxYkiK6g%40mail.gmail.com.