Procedure for hydrotest of pipeline GRE (UNDERGROUND)

243 views
Skip to first unread message

Benaouda Mezrar

unread,
Aug 3, 2022, 4:21:29 AM8/3/22
to Materials & Welding
hi expert 

could anyone have a procedure for HYDROTEST pipeline GRE 

thanks



Satyaprakash Soni/Infrastructure Solutions-MEP/MUM

unread,
Aug 3, 2022, 11:22:20 PM8/3/22
to material...@googlegroups.com
hope this works....

Thanks & Regards,
Satyaprakash Soni,Manager - QA/QC,Mobile +91-9892649099


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6e6313e0-c520-4df4-bf97-e08e17c4ab26n%40googlegroups.com.

****---------------------------**** 
Disclaimer : The information contained in this e-mail (including any attachments) is privileged and confidential. If you have received it by mistake please notify the sender by return e-mail and permanently delete this e-mail and any attachments from your system. Any dissemination, use, review, distribution, printing or copying of this message in whole or in part is strictly prohibited. Please note that e-mails are susceptible to change. Voltas Ltd. (including its group companies) shall not be liable for the improper or incomplete transmission of the information contained in this communication nor for any delay in its receipt or damage to your system. Voltas Ltd. (or its group companies) does not guarantee that the integrity of this communication has been maintained or that this communication is free of viruses, interceptions or interference.

Hydro Testing Procedure for Bondstrand GRE and GRV Pipe.pdf

Mohd Siraj

unread,
Sep 1, 2022, 2:30:05 AM9/1/22
to Materials & Welding

hi, Mr denaouda,

you can refer procedure provided and the last pl contact pipe mfg for final pressure and holding.(i think who is mfg CPI,oman ?)

there is two one test is strength test of 4 hr and second is a leak test of 24 hr at design or 1.1 design.

regards,
Siraj.

Benaouda Mezrar

unread,
Sep 1, 2022, 1:21:04 PM9/1/22
to material...@googlegroups.com
could you explain more sir or if you have a (document / standards) please send it to me may be it will help me  

thank you a lot sir 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages