Difference between Certificate of compliance and Certificate of conformance

4,481 views
Skip to first unread message

Idris Mohiuddin

unread,
Jan 10, 2011, 7:29:03 AM1/10/11
to material...@googlegroups.com
Dear Experts,
 
Please share your comments for the following query:
 
Difference between Certificate of compliance and Certificate of conformance
Regards,
 
MIM

p_cha...@mail.bg

unread,
Jan 10, 2011, 10:06:31 AM1/10/11
to material...@googlegroups.com, material...@googlegroups.com

Dear Sir,

In terms of Sect.VIII, Div.1:

Certificate of compliance (U-3 form) is being issued for pressure vessels to be stamped with UM symbol.

Certificate of conformance refers to the manufacturing or assembling of pressure relief valves UV (UV-1 form) or of nonreclosing pressure relief devices UD (UD-1 form).

 

Regards Parvan Chavdarov

TÜV Rheinland IS GmbH

----- Цитат от Idris Mohiuddin (idri...@gmail.com), на 10.01.2011 в 14:29 -----

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

Suresh Babu

unread,
Jan 10, 2011, 10:01:39 AM1/10/11
to material...@googlegroups.com

 

A cert of compliance states that you have complied with the requirements

A cert of conformance states that product conforms to requirements.
 
Regards,
SURESH.



--

jignes...@linde-le.com

unread,
Jan 11, 2011, 2:09:17 AM1/11/11
to material...@googlegroups.com

Dear Mr. Idrish,

I like to share my views on this topic. I am assuming that query is being asked from PED perspective.

Certificate of Compliance : Document in which Manufacturer declares that products supplied are in compliance with requirements of the order, without inclusion of test results. (EN 10204 Type 2.1)


Certificate of Conformance - ( Certificate of Conformity) - Certificate issued by Notified Bodies ( NB) / Manufacturer, after successful compliance of conformity assessment modules to meet the ESR ( Essential Safety Requirements ) of the Directive.

Attaching extracts for further guidance.



With Best Regards,

Jignesh R Rana
Manager - QA & QC

Linde Engineering India Pvt. Ltd.
38, Nutan Bharat Society, Alkapuri, Vadodara 390007, India
Tel.: +91 265 3056789, Fax: +91 265 2335213 , Mobil:  +91 90999 86019
jignes...@linde-le.com, www.linde-india.com

This e-mail is confidential. If you are not the intended recipient, please notify us immediately. You should not disclose its contents to any other person nor use it for any purposes.





Suresh Babu <suresh...@gmail.com>
Sent by: material...@googlegroups.com

10/01/11 20:31


To
material...@googlegroups.com
cc
Subject
Re: [MW:9173] Difference between Certificate of compliance and Certificate of conformance


certificate_of_conformity.pdf
COC - Wikipadia.pdf
Reply all
Reply to author
Forward
0 new messages