SAW consumable for API 5L X70 pipe joint

44 views
Skip to first unread message

Chintan

unread,
Jan 30, 2020, 4:21:51 AM1/30/20
to Materials & Welding
Dear Expert

Kindly advice on suitable flux and wire combination for x70 pipe
Joint type pipe to pipe cs
Pwht not applicable
Impact test not required

Thank you

meisam shokri arfaei

unread,
Feb 4, 2020, 11:06:30 AM2/4/20
to material...@googlegroups.com
Dear Chitan,

Depending on your WPS and welding parameters, too many SAW wire/flux combinations could be used. Normally, AWS A5.23 - EA2 (S2Mo) or EM12 (S2) or EM12K (S2Si) wires in combination with different AB (Aluminate Basic) fluxes which could provide F8AX-EA2 mechanical properties would be suitable for you.

For more details, you have to provide your WPS & parameters then consult with your consumable manufacturer.

Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6cf1c290-d520-4788-9f83-566188fee35b%40googlegroups.com.


--
M. Shokri Arfaei
ASNT NDT Level III
International Welding Engineer





Chintan

unread,
Feb 11, 2020, 10:53:50 PM2/11/20
to Materials & Welding
Thanks for info

Sharing result of my PQR

I run PQR with EH12k & neutral flux & got F8A3 mechanical property