Can any one explain with example of thickness qualifications - procedure.

Especially for combination of process with 19mm to 38mm thickness job welded. 
Explain me each and every step. 

Here I explain what I am understand that code. Weather it's wrong please explain.

Example. 

Job PQR thickness - 25.4mm
Process - GTAW (4mm)+ SMAW(21.4)

as per ASME sec IX, Qualifications range for GTAW 4mm --- min - 5mm, max- that is <19mm, 2t =8mm

Qualifications range for SMAW 21.4mm -- min-5mm, max- that is >19mm, 2T=2(25.4)=50.8mm

So..
The total thickness welded is 25.4(4+21.4)mm
Total thickness qualified is -=8+50.8=58.8mm


Is that correct or not.
If it wrong kindly give me a brief lesson to me.

Thank you
Ganesh
QC Welding

kingslygeo vargheese

unread,
Jul 25, 2022, 4:14:43 AM7/25/22
to material...@googlegroups.com
Dear Ganesh,

Job PQR thickness - 25.4mm                                 
Process - GTAW (4mm)+ SMAW(21.4)

as per ASME sec IX, Qualifications range for GTAW 4mm --- min - 5mm, max- that is <19mm, 2t =8mm      ----------------  GTAW - MAX  2t - 8 MM

Qualifications range for SMAW 21.4mm -- min-5mm, max- that is >19mm, 2T=2(25.4)=50.8mm                   ----------------  SMAW - Unlimited Thickness if PQR has been done with 3 layers of welding.

So..
The total thickness welded is 25.4(4+21.4)mm
Total thickness qualified is -=8+50.8=58.8mm                                                                                                ---------------   GTAW - 8 MM MAX  & SMAW  Unlimited thickness

image.png
image.png
Regards,
V.Kingsly Geo.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM0EmFJmvaHw6Nv%3DO%3Dm3-0N%2BGS-j0uED9QkRP%3DaXzE3%3DphOGEw%40mail.gmail.com.

Kannayeram Gnanapandithan

unread,
Jul 25, 2022, 11:30:41 PM7/25/22
to materials-welding
As per QW 452.1(b),  Deposited weld metal qualified thickness is , GTAW--8mm max,   SMAW- Max to be welded

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


srinivas rao

unread,
Jul 25, 2022, 11:30:54 PM7/25/22
to Materials & Welding
Dear  Ganesh, 
your undestanding was correct , go ahead.
 kindly ignore mail from Mr. V.Kingsly Geo. BCZ it is applicable for perfromace qualification.

Thanks 
Srinivas Rao

srinivas rao

unread,
Jul 26, 2022, 12:45:38 AM7/26/22
to Materials & Welding
kindly note that  QW-452 -is applicable only for Perfromance qualification , for procedure qualifcation thickness limits one has to follow QW-451 . hope this clarifys.

Thanks 
Srinivas Rao

kingslygeo vargheese

unread,
Sep 4, 2022, 10:02:51 AM9/4/22
to material...@googlegroups.com
Dear Srinivas,

Thanks for the clarification.

Regards
V.Kingsly Geo.