Lower - % Ferrite in Super Duplex Stainless Steel

66 views
Skip to first unread message

Chintan

unread,
Apr 29, 2021, 4:50:39 AM4/29/21
to Materials & Welding
Dear Expert, 

After Filling & Capping of  Weld Metal, During % Ferrite check via Feritoscope  values are showing less than requirement, How ever all other test i.e. Hardness, PMI etc. are well accepted. 
Kindly advice on  possible root cause as well as tips to achieve high Ferrite 
Please find below details for your quick ref. 
 Material Grade - SDSS -UNS s32760
Joint type -Pipe - Butt weld - 18 mm thick 
Welding Process - GTAW + SMAW 
Welding Consumable - ER 2594 + E 2594-15
% Ferrite - GTAW ( Root ) - 35%, SMAW ( Capping) - 25 -28 %, Base metal - 35to 40%, HAZ - 32 to 35% 
% Ferrite - Spec Req - 30  to 70%
Inerpass mentained - 100°C for GTAW, 120°C for SMAW
Heat input - GTAW - 0.8 to 1 KJ/mm
SMAW - 1.2 KJ/mm

Ahmed Osman

unread,
Apr 29, 2021, 6:27:41 AM4/29/21
to Materials & Welding
Dear Friend ,

try to replace E 2594 by E2595 .. it have W element which is promoting ferrite

Best Regards ,
ENG. Ahmed Osman

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6e8220cb-cdad-455d-b466-5cea0e6b4290n%40googlegroups.com.

Shyamal Das

unread,
May 3, 2021, 5:47:41 AM5/3/21
to material...@googlegroups.com
Hi

Please check the  shielding Gas 
Argon + 2 % Nitrogen  purity levels 
purging gas  100 percent Argon . Better to control with less than 100 ppm
You should have purge monitor with least count .001 

Nitrogen also play important role is Austentic and ferrtic phase distribution .

Kr

Das 


Alcindo Jardim

unread,
May 4, 2021, 6:37:05 AM5/4/21
to material...@googlegroups.com
Some results indicate that it is not just the shielding / purge gas that is interfering. The ferrite in the base metal is also off limits. I suggest investigating the factors further. it may be that the base metal is not within the standards, and the heat imput may also be high, changing the transformation kinetics. Run more tests before making the next weld.