Dear Experts.

                      could we follow ASME section 9 or AWS D1.1  for the structural steel welding qualification? please explain.

--
K. SARAVANAN. BE, ME (WELDING TECHNOLOGY)
     WELDING ENGINEER,
     BLACKCAT ENGINEERING  WLL,
     DOHA ,QATAR.
     MOBILE: +974-77466433. INDIA- +91 8939999299.

Rajendra Jadhav

unread,
Mar 13, 2017, 9:23:44 AM3/13/17
to material...@googlegroups.com

AWS D1.1

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALhxBzivrAMx4zTYJEtOb-jm6vEAxsVTm%3D%3DNrUNo6Z6s4Kme3Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Hareesh K V

unread,
Mar 13, 2017, 10:37:10 PM3/13/17
to materials-welding

Dear Mr.Saravanan,

The choice of the code cannot be decided in this way.
This depend on your specification and the design code. This can be easily decided by a designer and should have a written documentation between the client, the Designer and the Contractor.

Regards,

Hareesh K V
8547859202

--

Firdaus Awie

unread,
Mar 13, 2017, 10:37:17 PM3/13/17
to material...@googlegroups.com
Dear K.Saravan,

Can you give details what exactly do you want to ask?. AWS D1.1 is a reference code for Structural Steel procedure. Of course it can.

Sent from my iPhone
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.

Perumal Govindan

unread,
Mar 13, 2017, 10:50:03 PM3/13/17
to material...@googlegroups.com

Dear Saravanan,
Construction codes are normally indicated in the Project Specification or FEED documents, data sheets, PMS and GAD's.

In case if it is not there in the above documents,  prepare a QC Procedure or Method Statement for fabrication of structural works indicating AWS D1.1 as a construction code, submit to Client for approval.

Regards
P Govindan

SARAVANAN KRISHNAN

unread,
Mar 14, 2017, 12:50:04 AM3/14/17
to material...@googlegroups.com
Gents.
 oil and gas field structural welding which code we should follow?Ex pipe supports ladder hand rails..etc
            My suggestion  same the above designer and contractor it defense. suppose civil construction we should follow the AWS D1.1 /wps qualification,in the same manner in oil and gas field to be follow the designer and contractor .
 

On Mon, Mar 13, 2017 at 4:53 PM, 'Firdaus Awie' via Materials & Welding <material...@googlegroups.com> wrote:
Dear K.Saravan,

Can you give details what exactly do you want to ask?. AWS D1.1 is a reference code for Structural Steel procedure. Of course it can.

Sent from my iPhone

On 13 Mar 2017, at 8:13 PM, SARAVANAN KRISHNAN <saravweldingengineer@gmail.com> wrote:

Dear Experts.

                      could we follow ASME section 9 or AWS D1.1  for the structural steel welding qualification? please explain.

--
K. SARAVANAN. BE, ME (WELDING TECHNOLOGY)
     WELDING ENGINEER,
     BLACKCAT ENGINEERING  WLL,
     DOHA ,QATAR.
     MOBILE: +974-77466433. INDIA- +91 8939999299.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/502C02E2-E22E-4179-AEB3-69CAE839A34C%40yahoo.com.

For more options, visit https://groups.google.com/d/optout.

irfan...@gmail.com

unread,
Mar 18, 2017, 10:37:44 PM3/18/17
to material...@googlegroups.com

Generally ASME is referred to process piping and AWS is referred to structural steels which includes Platforms, supports, handrails
Also refer to your client specification for governing code they prefer.
In general piping specification are addendum to Asme B31.3 and structural steels specification are addendum to AWS D1.1

Irfan.M
00974-55149121



Sent from my Huawei Mobile
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALhxBzj7BGhVBDYcBCe8Ac%3D5QGpHxmkNwRxqFuR6CJKC7MMUkQ%40mail.gmail.com.

Kannayeram Gnanapandithan

unread,
Mar 19, 2017, 1:19:10 AM3/19/17
to materials-welding
If it is non pressure parts which is integral part of pressure, then follow ASME sec9. if it is structural like beams ,columns for boilers and others which is not directly attached to pressure parts, follow AWS D1.1

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Tue, Mar 14, 2017 at 8:28 PM, irfan...@gmail.com <irfan...@gmail.com> wrote:

Generally ASME is referred to process piping and AWS is referred to structural steels which includes Platforms, supports, handrails
Also refer to your client specification for governing code they prefer.
In general piping specification are addendum to Asme B31.3 and structural steels specification are addendum to AWS D1.1

Irfan.M
00974-55149121



Sent from my Huawei Mobile


-------- Original Message --------
Subject: Re: [MW:26205] ASME AND AWS D 1.1 clarification for wps qualificatioon
From: SARAVANAN KRISHNAN
To: materials-welding@googlegroups.com
CC:


Gents.
 oil and gas field structural welding which code we should follow?Ex pipe supports ladder hand rails..etc
            My suggestion  same the above designer and contractor it defense. suppose civil construction we should follow the AWS D1.1 /wps qualification,in the same manner in oil and gas field to be follow the designer and contractor .
 
On Mon, Mar 13, 2017 at 4:53 PM, 'Firdaus Awie' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear K.Saravan,

Can you give details what exactly do you want to ask?. AWS D1.1 is a reference code for Structural Steel procedure. Of course it can.

Sent from my iPhone

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

Dinesh Somwanshi

unread,
Mar 19, 2017, 3:17:55 AM3/19/17
to material...@googlegroups.com

The acceptance of Pqr .Wps is defined in client specs.

Thanking You,

With Regards..
Dinesh V Somwanshi
Api 570, Cswip 3.1,Bgas 2
Authorised Certified Piping, Welding, Painting Inspector.
00919881344135

Naskabir Vengassery

unread,
Mar 19, 2017, 6:25:23 AM3/19/17
to Materials & Welding
Dear Saravanan,
 Your query was "could we follow ASME section 9 or AWS D1.1  for the structural steel welding qualification? please explain." are you asking about procedure qualification or performance qualification ?
1) if  Procedure qualification- as explained earlier by Hareesh, the designer has to specify what is the governing code. (for structural steel works AWS D1.1 is generally followed)
2) if  Performance qualification- the governing design code/ approved WPS has to be followed.

Note: if you have previously qualified welders in the same range of variables but qualified on a different code, then you may approach the end user to accept them without a new qualification 
Good luck.

Naskabir V
Doha

Agustin Jimenez

unread,
Mar 19, 2017, 9:10:45 AM3/19/17
to material...@googlegroups.com
If you PQR cover the parameter according AWS D1.1 them you can make WPS D1.1 from it PQR.


Agustin Jimenez +584167801321


-------- Mensaje original --------
De: Naskabir Vengassery <nask...@gmail.com>
Fecha:2017/03/19 04:19 AM (GMT-04:00)
Para: Materials & Welding <material...@googlegroups.com>
Cc:
Asunto: [MW:26231] Re: ASME AND AWS D 1.1 clarification for wps qualificatioon
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ccd28688-56fa-4bc0-94cc-6f2dd415471c%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages