Equivalent material for Steel Grade S355G1 (+N)

922 views
Skip to first unread message

Bathula Raghuram (Mumbai - PIPING)

unread,
Aug 13, 2008, 12:06:37 AM8/13/08
to material...@googlegroups.com

In additional to variation in chemical composition (thou UTS/YS or more or less equal) G1 +N has CVN impact testing with min 50J @-20 °C and value of CEQ is restricted to 0.43 Vs 0.45/0.47 in case of JR material.

You need to prepare a comparison chart tabulated (one similar is attached for your ready reference) with all the values, and analyse where you are deviating and what is your end requirement (is there any CVN impact requirement or any CE restriction in client spec? etc.)

 
Probably this way you can get approval from your client with an additional testing such as CVN impact.

 

 


From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of SENTHILKUMAR SWAMINATHAN
Sent: Tuesday, August 12, 2008 10:14 PM
To: Engineering
Subject: [MW:1022] Using Following Material

 

Hi,

As per Dwg, I have to use BS EN 10225 Part-III, Steel Grade S355G1 (+N), where as available material BS EN 10025 Part-2 Steel Grade S355JR is there any record to use available material.  

 

Norsok M-120 says YO3 S355N1 equivalent but no same material. Please help me.

 

Regards,

S.Senthilkumar



Material_Comparison_List.pdf

SENTHILKUMAR SWAMINATHAN

unread,
Aug 13, 2008, 2:03:32 AM8/13/08
to material...@googlegroups.com
Hi Raghuram,
Thank you, client may not agree because difference is more than 50% change in impact value.
 
Regards,
S.Senthilkumar

--- On Wed, 13/8/08, Bathula Raghuram (Mumbai - PIPING) <R.Ba...@ticb.com> wrote:
From: Bathula Raghuram (Mumbai - PIPING) <R.Ba...@ticb.com>
Subject: [MW:1024] Equivalent material for Steel Grade S355G1 (+N)
Date: Wednesday, 13 August, 2008, 9:36 AM

In additional to variation in chemical composition (thou UTS/YS or more or less equal) G1 +N has CVN impact testing with min 50J @-20 °C and value of CEQ is restricted to 0.43 Vs 0.45/0.47 in case of JR material.

You need to prepare a comparison chart tabulated (one similar is attached for your ready reference) with all the values, and analyse where you are deviating and what is your end requirement (is there any CVN impact requirement or any CE restriction in client spec? etc.)

 
Probably this way you can get approval from your client with an additional testing such as CVN impact.

 

 


SENTHILKUMAR SWAMINATHAN


Sent: Tuesday, August 12, 2008 10:14 PM
To: Engineering
Subject: [MW:1022] Using Following Material

 

Hi,

As per Dwg, I have to use BS EN 10225 Part-III, Steel Grade S355G1 (+N), where as available material BS EN 10025 Part-2 Steel Grade S355JR is there any record to use available material.  

 

Norsok M-120 says YO3 S355N1 equivalent but no same material. Please help me.

 

Regards,

S.Senthilkumar




 