Dear All,

Can we able to make revision of WPQR ? which is made as per ISO 15614-1.

I am not sure about this.

There are some points which is not added in the WPQR, so I want to add these point.

I know the requirement of ASME section IX. as per IX we can not able to make revision of PQR only amendment can be make.

Thank you in advance.

Vijay Katkar

george....@gr.bureauveritas.com

unread,
Oct 30, 2015, 11:35:54 AM10/30/15
to material...@googlegroups.com

A PQR is never revised.
A WPS yes
best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Joseph

unread,
Oct 31, 2015, 1:18:46 AM10/31/15
to material...@googlegroups.com
Hi, you can supplement it with a additional sheet containing the data you want to include.

Sent from my iPad
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/OF6B40F6AF.0E07C239-ONC2257EEE.004EDB53-C2257EEE.004EE2C8%40LocalDomain.
For more options, visit https://groups.google.com/d/optout.
Reply all
Reply to author
Forward
0 new messages