Hi All,

Kindly suggest on following points.
  • What is difference between ISR & DHT and why it is important?
  • DHT can be performed in lue of ISR? If yes, what kind of precautions need to be taken care?
  • DHT will have less cost and less time consuming cpmpared to ISR?

Br,
Chandan

Viral Talati

unread,
May 29, 2020, 11:45:39 AM5/29/20
to material...@googlegroups.com
You are advised to refer API RP 934 C 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP2dnyGhy8qgvqONkcVcEe7_KwbWpH44RCAnLgqfXFqnb7CJ9Q%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages