RT film size required

111 views
Skip to first unread message

anand gupta

unread,
Mar 19, 2020, 7:11:01 AM3/19/20
to Materials & Welding
Dear all

Please confirm the width of RT film as per ASME Sec VIII. 

Regards 

A p gupta 

George Dilintas

unread,
Mar 30, 2020, 1:15:22 AM3/30/20
to material...@googlegroups.com
There is no requirement for width. 
There is no requirement for the length of a single film.
There is a requirement for the minimum length to be radiographic in case of spot RT (read UW-52).
Each one welder's job has to be RTed.
One spot for each 15 meters of weld has to be RTed.
The min length of the spot is 150 mm

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/264284656.692462.1584613280413%40mail.yahoo.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis