TEST COUPON ASME SEC IX

116 views
Skip to first unread message

Elavarasan Mech

unread,
Mar 28, 2025, 11:00:41 PM3/28/25
to material...@googlegroups.com
Please clarify below 
As per ASME SEC IX can we use 14mm plate machined to 8 mm plate for WPS & WQT qualification.please guide me 
 
Regards 
ELAVARASAN 

Venkatesh Mech

unread,
Mar 29, 2025, 2:37:18 AM3/29/25
to material...@googlegroups.com
Hi elavarasan,
Can you elaborate whether you have to machine 14mm plate to 8 mm for welding, or you have to make 8mm plate instead of 14mm. 

Select the weld plate thickness based on your casting weld depth .

Incase your casting weld depth requirement is more than 2 inch better you can for 40mm plate so that you can weld as much as the depth as standard requirement, make sure you have to get approval incase you are doing major weld on the part based on customer requirement.

Regards,
Venkateshwaran 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ym4-UGqb6tprYjv66ifU7fan--MHmyUneojUPdVkv44Fg%40mail.gmail.com.

venkateswara reddy Desireddy

unread,
Mar 29, 2025, 2:37:41 AM3/29/25
to material...@googlegroups.com
Yes we can use. Write in as Run sheet 16mm plate machined to 8 mm.

--

raj kumar

unread,
Mar 29, 2025, 2:37:45 AM3/29/25
to material...@googlegroups.com
Wps 
As per my opinion, If qualified 8mm plate min 5mm and Max 2T, weld metal -2t.


On Sat, 29 Mar, 2025, 08:30 Elavarasan Mech, <elavaras...@gmail.com> wrote:
--

Elavarasan Mech

unread,
Mar 29, 2025, 2:58:25 AM3/29/25
to material...@googlegroups.com
dear sir 
 Actual project thickness :9mm ( impact required)PED
we have 14 mm thick plate SA516 G70 .if considered impact requirement as per ASME SEC IX ( WPS QUALIFICATION )we need minimum base mental thickness  9mm .we plan to weld 14mm plate decrease the thickness to 8mm .still my WPS qualified with impact 8mm To 16 mm.
My consideration is machined plate acceptable or not  which standard I need to refer 


ELAVARASAN


Parminder Singh

unread,
Mar 29, 2025, 7:47:23 AM3/29/25
to material...@googlegroups.com
Yes, You can machine the Plate. 
Prepare the Welding Running Sheet and mention 14 mm Plate machined to 8 mm Plate. 

then the groove weld qualification will be 8-16 mm for impact test and 1.5 - 16 mm without impact test

Mohd Siraj

unread,
May 15, 2025, 9:49:25 AM5/15/25
to Materials & Welding
yes, joint design shall mentioned on PQR.accodingly WPS shall be prepared and records.