Differnce between A350 LF1 and LF2

1,501 views
Skip to first unread message

Himan Nikdin

unread,
Apr 11, 2017, 11:28:59 AM4/11/17
to material...@googlegroups.com

Dear Experts,

Good Day!!


I have query regarding SA350 LF1 and LF2, as you can compare the chemical composition of two grades, there are no difference between two grades;


but you can see the major difference between impact test temperature, what is the reason for this major difference as in SA-350 there is no major heat treatment requirements.


also what is the reason for difference between impact test temperature of LF2 Class 1 and class 2?

thanks indeed if you share your valuable ideas.


Regards,

Himan Nikdin

George Dilintas

unread,
Apr 14, 2017, 1:35:01 AM4/14/17
to Meghanadh K
Grain Size

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/DB6PR0902MB1717D3B2FCC67FCBD4651C9C9E000%40DB6PR0902MB1717.eurprd09.prod.outlook.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

Himan Nikdin

unread,
Apr 14, 2017, 8:26:04 AM4/14/17
to material...@googlegroups.com

Dear George


I do not disagree with you, but different grain size is achievable by different chemical composition and/or heat treatment, but I can't find any different chemical composition or heat treatment.


Regards,

Himan Nikdin


From: material...@googlegroups.com <material...@googlegroups.com> on behalf of George Dilintas <dili...@gmail.com>
Sent: Wednesday, April 12, 2017 10:44:39 PM
To: Meghanadh K
Subject: Re: [MW:26403] Differnce between A350 LF1 and LF2
 
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40BLmdZFddAfakdzAjVprEX1VN5rCS%2BsVt%2BdCujfBtJ2%2Bg%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages